Isu-hagaajinta habka daaweynta kuleylka ee GH690 biibiile daawaha ah
Tuulada dalada ah ee loo yaqaan '690 tube alloy' ee loo isticmaalo tuubada wareejinta kuleylka dhaliyaha uumiga ee warshadda tamarta nukliyeerka waxay xambaarsan tahay daxalka heerkulka sare, cadaadiska sarreeya iyo dhexdhexaadka biyaha, cabbirka hadhuudhka daloolka ah, kala-goynta CR-da ee is-dhexgalka, carbide-ka isku-xidhka ah iyo xooggeeda ku saabsan fiirsashada walaaca.
Saamaynta tacliimeed waa cunsur muhiim ah oo saameysa daxalka iyo u adkaysiga daxalka walxaha ee qalabka. Marka lagu daro in si adag loo xakameeyo halabuurka, habka daaweynta kuleylka ee macquulka ah ayaa baabi'in kara saameynta arrimahan ku leeyihiin guryaha maaddada.
Faa'iidada iyo saameynta ayaa muhiim ah.
Qaadashada microstructure-ka shisheeyaha Inconel 690 oo dhammeystiran sida sheyga tixraaca, xallinta xalka iyo kuleylka daaweynta kuleylka ah (daaweynta TT) ee tubbada daawaha ah ee GH690 ee gudaha iyadoo la raacayo xaalado kala duwan.
Cilmi baaris ayaa la sameeyay; Saamaynta cabbiraadaha geeddi-socodka ee cabbirka hadhuudhkeeda, qaab-dhismeedka carbide ee xadka iyo aagga Cr-saboolka ah ayaa lagu falanqeeyay habab lagu garto sida OM, SEM iyo TEM. natiijada ayaa muujineysa:
(1) Qaybinta hadhuudhka ee dhammaystirka Inconel 690 dhuumaha dibedda waa mid aan sinnayn, celceliska cabbirka hadhuudhku waa qiyaastii 23μm, tirada miraha leh cabbirka badarka 7 ilaa 10 ayaa ugu weyn. Carbides xudduudda badiyaa way fiican yihiin.
Qaybaha TiN waxaa loo qaybiyaa si isdaba-joog ah waxaana jira qaybo badan oo TiN-weyn ah. Waxaa jira gobol Cr-sabool ah oo ballaciisu yahay 200nm oo u dhow soohdinta hadhuudhka.
(2) Inta lagu gudajiro geedi socodka daaweynta xalka ee tuubada alloy ee GH690 ee gudaha, maadaama heerkulka xalka uu kordhayo, badarka macdanta ah ayaa sii kordheysa, iyo tamarta firfircoonida koritaanka waa 265kJ / mol. Marka heerkulka xalka adag uu dhaafo 1100 ℃.
Waqtigaan, koritaanka hadhuudhka ayaa sii muuqda, iyo saameynta waqtiga ku haynta cabirka miraha sidoo kale waxay noqoneysaa mid muhiim ah.
(3) Ka dib markii tuubbada daawaha ah ee GH690 ee gudaha lagu daaweeyo TT iyada oo la raacayo xaalado geedi socod kala duwan, carbides xuduuda badarka inta badan waxay u muuqataa ganaax iyo kala firidhsan, ganaax iyo semi-joogto ah, qalafsan iyo semi-joogto ah, iyo qalafsanaan iyo kala firidhsan.
Nooca xaaladda qaybinta. Marka xuduudaha geeddi-socodka ee daaweynta TT ay yihiin 680 ℃ / 10 ~ 20h, 715 ℃ / 10 ~ 20h, 750 ℃ / 5 ~ 15h, carbides xudduudda hadhuudhka waxaa loo qaybiyaa si wanaagsan semi-joogto ah.
(4) Iskucelceliska cabbirka hadhuudhka iyo cabbirka hadhuudhka ee loo qaybiyo tuubbada daloolka GH690 ee gudaha ka dib marka lagu daweeyo xalka 1090 ~ 1110 ℃ / 5min waxay u dhowdahay kuwa qalaad ee Inconel 690 tuubbo dhammaatay. Kadib 715 ℃ / 10h ama 15h
Daaweynta TT ka dib, qaab dhismeedka carbide xuduudaha iyo sifooyinka aagga Cr-saboolnimada ee aaladda tuubbada guryaha ee GH690 waxay la mid tahay kuwa Inconel 690 ee tuubbada qalaad, laakiin cabirka iyo tirada walxaha TiN aad ayey u yar yihiin una yar yihiin.
Qaybta dambe, iyo fiirsashada ugu hooseysa ee Cr ayaa ka sareysa tan dambe, waxay ka caawineysaa hagaajinta iska caabbinta daxalka iyo u adkaysiga daxalka isugeynta ee aaladda. Qaab dhismeedka guud ee tuubbada daawaha ah ee GH690 ayaa ka fiican kan shisheeyaha ah ee Inconel 6
90 tuubooyin dhammeeyey.
(5) Isbarbardhiga dhameystiran ee astaamaha qaabdhismeedka 690 tuubooyin daawaha ah gudaha iyo dibedda, iyo iyadoo la tixgelinayo arrimaha ku saabsan wax soo saarka dhabta ah, waxaa lagugula talinayaa in habka ugu habboon ee daaweynta kuleylka ee tuubbada daawaha ah ee GH690 ay tahay 1090 ~ 111
0℃/5min+715℃/10~15h.
Fadlan hayso isha iyo cinwaanka maqaalkan si dib loogu daabaco: Isu-hagaajinta habka daaweynta kuleylka ee GH690 biibiile daawaha ah
Minghe Shirkadda Die Casting waxaa ka go'an in ay soosaaraan oo ay bixiyaan Qaybo ka ridaya tayo iyo waxqabad sare (biraha qaybo ka ridaya dhiman kala duwan inta badan ka mid yihiin Khafiifa-Wall dhinta ridaya,Hot ridaya die Cast,Kursiga Qabow Die Casting), Adeeg Wareeg ah (Adeegga Tartanka Dhimashada,Qalabka Mashiinka,Samaynta Furka, Daaweynta Dusha sare) .Caadi kasta oo Aluminium ah shubitaan, magnesium ama Zamak / zinc shubida iyo shuruudaha kale ee shubanka ayaa lagu soo dhaweynayaa inaad nala soo xiriirto.
Iyada oo ay gacanta ku hayaan ISO9001 iyo TS 16949, dhammaan geeddi-socodyada waxaa lagu fuliyaa iyada oo loo marayo boqollaal mashiinno shub ah oo dhimanaya, mashiinnada 5-dhidibka, iyo tas-hiilaadka kale, oo ka bilaabma qarxiyayaal ilaa mashiinnada dharka lagu nadiifiyo ee Ultra Sonic.Minghe ma ahan oo keliya qalab casri ah laakiin sidoo kale waxay leedahay xirfadle koox injineero khibrad leh, wadayaal iyo kormeerayaal si niyada macaamiisha ay u noqoto mid run ah.
Soo saaraha qandaraasle ee shubka dhinta. Awoodda waxaa ka mid ah qaybaha qabow ee aluminium ee qaybaha shubista laga bilaabo 0.15 lbs. illaa 6 rodol, isbeddel deg deg ah oo la dejiyay, iyo qalabaynta. Adeegyada qiimaha lagu daro waxaa ka mid ah sifaynta, gariirka, qashin-qubka, xabbadda toogashada, ranjiyeynta, dahaadhka, dahaadhka, isku-ururinta, iyo qalabaynta. Qalabka lala shaqeeyay waxaa ka mid ah alloysyada sida 360, 380, 383, iyo 413.
Zinc wuxuu u dhintaa caawinta naqshadeynta / adeegyada injineernimada isku mar. Soo saaraha gaarka ah ee saxda saxda ah ee looxyada. Daarayaasha yar-yar, cast-yada u dhinta cadaadiska sare, jilayaasha caaryada badan-slide, shubka caaryada caadiga ah, cutubka dhinta iyo kuwa madaxa-bannaan ee loo dhinto iyo daloolka dahaarka saanlan ayaa la soo saari karaa. Jilayaasha waxaa lagu soo saari karaa dherer iyo ballac ilaa 24 gudaha. +/- 0.0005 gudaha. Dulqaad.
ISO 9001: soo saaraha shahaadada leh ee loo yaqaan 'cast cast magnesium', Awoodaha waxaa ka mid ah dhimista cadaadiska sare ee magnesium oo loo ridayo ilaa 2015 ton qol kulul & 200 ton oo qol qabow ah, naqshadeynta qalabka, nadiifinta, wax u sameynta, mashiinada, budada & dareeraha rinjiyeynta, QA buuxda oo leh awooda CMM , ururinta, baakadaha & gaarsiinta.
ITAF16949 la xaqiijiyay. Adeeg Dheeraad Dheeraad ah Ayaa Kujira maalgelinta maalgelinta,ciida ciid,Dabaaldeg Shaqo, Casting Foam Fost,Khadka Centrifugal,Dabka Vacuum Casting,Qaab Joogtada ah, Awoodda waxaa ka mid ah EDI, kaalmada injineernimada, qaabeynta adag iyo ka shaqeynta heerka labaad.
Warshadaha Kabka Qaybaha Daraasada Kiiska ee loogu talagalay: Gawaarida, Baaskiiladaha, Diyaaradaha, Qalabka muusikada, Biyaha, Qalabka indhaha, Dareemayaasha, Moodooyinka, Aaladaha elektarooniga ah, Xiritaanka, Saacadaha, Mashiinnada, Mashiinnada, Qalabka guryaha, Dahabka, Jigs, Telecom, Laydhka, Qalabka Caafimaadka, Qalabka Sawirka, Robotyo, farshaxanno, qalabka codka, Qalabka isboortiga, Qalabaynta, Caruurta iyo waxyaabo kale oo badan.
Maxaan kaa caawin karnaa inaad sameyso marka xigta?
Tag bogga hore ee loogu talagalay Shiinaha dhinta Casting
→Qeybaha kabkaOgow waxaan soo qabanay.
Tips Tilmaamaha Halaasiga ah ee Ku Saabsan Adeegyada Cast Cast
By Soo saaraha Minghe Die Casting | Qeybaha: Maqaallo waxtar leh |Waxyaabaha Tags: Casting Aluminium, Tuurista Zinc, Ridaya Magnesium, Qalitaanka Titanium, Qalabka birta ee birta, Naxaas naxaas ah,Raxaama Naxaas,Video Tuuraya,Taariikhda Shirkadda,Calaamadda Aluminum Die Casting | Faallooyinka Off