Faa'iidooyinka iyo Faa'iido-darrada Geeddi-socodka Daarista Aluminium
Sababtoo ah walxaha kala duwan ee koox kasta oo aluminium aluminium ah, sifooyinka jirka iyo kiimikada ee aaladaha ayaa ka duwan. Habka crystallization sidoo kale waa ka duwan yahay. Sidaa darteed, waa in loola jeedaa astaamaha aluminium aluminium. Xulashada macquul ah ee habka loo shubay. Si looga hortago ama loo yareeyo dhacdooyinka cilladaha wax lagu ridayo ee ku jira xadka la oggol yahay, si loo wanaajiyo shubka.
Waxqabadka Alxanka Daawaha Aluminium
Waxqabadka aluminium aluminium waxqabadka. Badanaa waxaa loo fahmay inay tahay isku-dar ah sifooyinkaas kuwa ugu caansan geedi socodka buuxinta sifooyinka, crystallization iyo qaboojinta, sida dheecaanka, yaraanshaha, ciriiriga hawada, cadaadiska tuurista, iyo nuugista hawada. Astaamahan aluminiumku waxay kuxiran yihiin isku-darka isku-darka. Laakiin waxay sidoo kale la xiriirtaa sababaha wax loo tuurayo, kakanaanta caaryada kuleylka kuleylka kululeeyaha, nidaamka kicinta ee shubashada, iyo qaabka albaabka.
(1) Dareenka
Dheecaanku wuxuu loola jeedaa awooda sifooyinka buuxinta dareeraha. Dareeraha ayaa go'aaminaya in daawaha uu tuuri karo shubisyo adag. Waxaa jira arrimo badan oo saameeya xisaabaadka. Waxyaabaha ugu muhiimsan waa halabuurka, heerkulka, iyo walxaha adag ee biraha oksaydhka, iskudhafka biraha iyo wasakhda kale ee dareeraha daawaha ah, laakiin sababaha ujeeddada dibadeed waa heerkulka daadanaya iyo cadaadiska socodka (oo inta badan loo yaqaanno madaxa duritaanka oo isku ururay).
(2) Qandaraas
Shrinkage waa mid ka mid ah astaamaha ugu muhiimsan ee aluminium aluminium la tuuray. Daawaha wuxuu u qaybsan yahay saddex marxaladood oo ka bilaabma dareeraha ku shubmaya ilaa adkeynta illaa uu ka gaarayo heerkulka qolka. Waxay yihiin hoos u dhac dareere ah, yaraanshaha adkeynta iyo yaraanshaha xaalada adag. Hoos u dhigidda aaladda waxay leedahay saameyn go'an oo ku saabsan tayada ridaya. Waxay saameyn ku yeelaneysaa cabirka yaraanshaha godka ridaya, sameynta dildilaaca culeyska fekerka iyo isbedelka cabirka. Yaraanshaha berkelium-ka joogtada ah ee degdega ah wuxuu u qaybsan yahay yaraanshaha jirka iyo yaraynta qadka toosan. Soo-saarista dhabta ah, yaraynta qadka toosan ayaa guud ahaan loo isticmaalaa si loo hagaajiyo yaraanshaha isku-darka dahabiga. Aluminium Aluminium cabbirka yareynta. Badanaa waxaa lagu muujiyaa boqolley ahaan, oo loo yaqaan yareynta.
Ction foosha jirka
Fuujinta jirka waxaa ka mid ah foosha dareeraha iyo foosha oo adkaata.
Dareerida dareere daawaha ka shubaysa si ay u adkeynta. Dhamaadka adkeynta, waxaa jiri doona yaraanshaha macroscopic ama microscopic ee dhinaca Vietnamese. Nooca noocan ah ee macruufka ah ee ay keento yaraanshaha ayaa u muuqda isha qaawan waxayna u qaybsan tahay yaraanshaha isku urursanaanta iyo yaraanshaha qeyb ahaan. Dhexroorkii godka godka yaraaday ee yaraaday waa weyn yahay oo urursan yahay. Waxaana lagu qaybiyaa qaybta sare ee shubista ama baraha kulul ee dusha sare. Godadka yaraanshaha ee kala firidhsanaa way kala firidhsan yihiin oo way fiican yihiin. Intooda badan waxaa loo qaybiyaa dhidibka shubka iyo kala-goysyada kulul. Godadka microscopic-ka waa ay adag tahay in lagu arko isha qaawan. Inta badan godadka yaraanshaha microscopic-ka waxaa lagu qaybiyaa xuduudaha hadhuudhka ama inta udhaxeysa dendrites-ka dendrites.
Yareynta iyo dabacsanaanta ayaa ka mid ah cilladaha ugu waaweyn ee tuurista. Sababta ayaa ah in foosha dareeraha ay ka weyn tahay qandaraaska qaranka. Inta lagu jiro wax soo saarka, waxaa la ogaaday in tuubada aluminiumka ee kala-soocista adkeynta ay ka yar tahay. Noocyada badan ayaa sameeya godadka yaraanshaha Leizhong. Hubi baaxadda xiidmaha. The crystals ka badan ayaa sameeya daloolada yaraanshaha ee kala daadsan. sidaa darteed. Naqshadeynta, aluminium aluminium ah oo dahaarka leh waa inuu u hoggaansamo mabda'a adkeynta isku xigxiga. Yaraanshaha jirka ee kabka daabacan inta lagu jiro adkeynta gacanta dareeraha ah waa in lagu daro dareeraha daawaha. Daloolada yaraanshaha iyo dabacsanaanta ayaa ku urursan qatarta sare ee shubka. Looxanka aluminium ee aluminium ee u nugul firidhsan iyo dabacsan. Tirada rakibaadda 100-deked ayaa ka badan kuwa godadka yaraanshaha dhexe. Oo waxaad dhigtaa bir qabow meesha kristantarradeedu ka soo baxaan si loo kordhiyo heerka qaboojinta maxalliga ah. Ka dhig mid sii xoojiya isla waqtiga ama si dhakhso leh.
Ine Yaraynta khadka
Cabirka hoos u dhigista xariiqda ayaa si toos ah u saameyn doonta tayada loo shubay. Nidaamku wuu yaraadaa wuuna casuumaa. Joogitaanka aluminium-tuurka si loo soo saaro dildilaacyo iyo walbahaar ayaa sidoo kale ka sii weyn: cabbirka iyo qaabka jilayaasha ayaa sii weynaanaya qaboojinta ka dib.
Noocyada kala duwan ee aluminium ee loo yaqaan 'cast aluminium', waxaa jira heerar kala-sooc ah oo kala-goysyada ah, isla daawahaasna waa la daabacay. Shubay waa ka duwan yahay. Heerka yaraanshaha sidoo kale wuu ka duwan yahay. Isla shubay Heerka yaraanshaha ee dhererkiisa, ballaciisa iyo dhererkiisuba sidoo kale waa ka duwan yahay. Waa in lagu go'aamiyaa iyadoo loo eegayo xaaladda gaarka ah.
(3) Dildilaac kulul
Dhacdooyinka dildilaaca kulul ee aluminium tuurista ayaa badanaa sabab u ah ciriiriga yaraanshaha ee jilayaasha oo ka batay xoogga isku xidhka u dhexeeya miraha birta. Intooda badani waxay ka dhacaan xuduudaha hadhuudhka. Waxaa laga arki karaa jabka dillaaca in biraha meelaha dillaacsan ay badanaa oksidheeyaan oo lumiyaan dhalaalkooda macdan. Dildilaacyadu waxay ku fidsan yihiin soohdinta hadhuudhka, oo leh qaab zigzag ah, dusha ballaadhan iyo cidhiidhi gudaha ah, qaarna waxay dhex galayaan dusha dhammaadka dhererka dusha.
Noocyada kala duwan ee aluminiumku waxay leeyihiin u janjeera kala duwanaan Tani waa sababta oo ah farqiga weyn ee u dhexeeya heerkulka kaas oo qaab dhammaystiran oo crystalline ah la sameeyay inta lagu gudajiray xoojinta aluminiumka aluminiumka ah iyo heerkulka xoojinta, ayaa sii weynaanaya hoos u dhaca alloy iyo u janjeera dilitaanka kulul, Xitaa isku nooca daawaha ayaa u janjeera dildilaac kulul kala duwan ay sabab u tahay caabbinta caaryada, qaab dhismeedka ridaya, habka shubidda iyo arrimo kale. Tallaabooyinka sida wasakhda tuurista dib-u-celinta ama hagaajinta tuurista aluminium aluminium ayaa badanaa loo isticmaalaa soo-saarka si looga fogaado dildilaaca aluminium-tuurka. Qaabka giraanta dildilaaca kulul waxaa badanaa loo isticmaalaa in lagu ogaado dildilaaca kulul ee tuurista aluminium.
(4) Cidhiidhi hawo ah
Hawada cidhiidhiga ah ee aluminium aluminiumka la tuuray waxaa loola jeedaa heerka ka-bax la'aanta tuubada nooca aluminium ee godka hoostiisa tallaabada gaaska cadaadiska sare leh ama dareeraha. Hawada cidhiidhiga ah ayaa dhab ahaantii tilmaamaysa heerka isukeenida iyo nadiifnimada qaab dhismeedka gudaha ee ridaya.
Isku-xirnaanta hawada ee aluminium aluminium la shubay waxay la xiriirtaa sifooyinka aaladda. Yaraanta kala duwanaanta isku-dhafka ee daawaha, ayaa u nugul yareynta soo-saarista. Isla mar ahaantaana, yaryar daloolada roobabku, waxay sare u qaadaan ciriiriga hawada ee isku-darka. Hawo-qabashada isla daawaha aluminium ee kabka ayaa sidoo kale la xiriirta habka loo shubay. Tusaale ahaan, hoos u dhigida heerkulka tuurista ee aluminiumka kabka la tuuro, oo birta qabow la dhigo si loo dardar galiyo heerka qaboojinta, iyo in la adkeeyo oo la caddeeyo in cadaadis la saarayo, iwm. hagaajin. Habka uur-qaadida ayaa sidoo kale loo isticmaali karaa in lagu xiro farqiga dheecaanka si loo hagaajiyo cidhiidhiga hawada ee ridaha.
(5) Culeyska fekerka
Cadaadiska tuurista waxaa ka mid ah seddex nooc oo walaac ah, walaaca isbeddelka wajiga iyo walwalka yaraanshaha. Sababaha keena walwalka kala duwan isku mid ma aha.
Hawo-qabad la'aanta aluminiumka la tuuray waxay la xiriirtaa sifooyinka aaladda. Waxyaabaha yar yar ee isku-dhafka alloy. U janjeera in la soo saaro geed baaruud baaruud sidoo kale waa yar yahay. Isla mar ahaantaana, waxay soo saartaa stomata yar. Haddii kale, cidhiidhiga hawada ee daawaha ayaa sarreeya. Hawo-qabashada isla daawaha aluminium ee kabka ayaa sidoo kale la xiriirta habka baaritaanka shubista. Sida hoos u dhigida heerkulka tuurista ee aluminium aluminium ah ee la tuuray, dhigista birta qabow si loo dardar galiyo heerka qaboojinta, iyo xoojinta iyo kristaylista cadaadiska, iwm. Cidhiidhiga gaaska ee ridaya ayaa sidoo kale lagu hagaajin karaa iyada oo la isku dhejiyo farqiga dheecaankiisu badan yahay iyadoo loo marayo habka daaweynta.
- Cadaadiska kuleylka. Cadaadiska kuleylka wuxuu u sabab yahay dhumucda qaybta aan sinnayn ee isgoyska qaababka joomatari ee kala duwan ee loo shubay. Qaboojinta ma aha sababo dhawr ah. Sameynta culeyska cadaadiska ee qaybta khafiifka ah waxay u horseedaa culeys haraaga ah ee ridaya.
- Kala-goynta culeyska. Cadaadiska isbeddelka wajiga ayaa u sabab ah isbeddelka wajiga ee qaar ka mid ah aluminium aluminium ah inta lagu jiro geedi socodka qaboojinta ka dib adkeynta. Cabirka aaga ku yaal dhamaadka ardaaga ayaa isbedelaya. Xubinta ugu weyni waa aluminium. Dhumucda gidaarka shubista ma sinna. Waxaa sababa isgoyska qaybo kala duwan waqtiyo kala duwan.
- Cadaadiska yaraanshaha. Marka tuurista aluminiumku yaraato, waxaa caqabad ku ah caaryada iyo udub-dhexaadka, taasoo keenta cadaadis kacsan. Cadaadiska noocan ahi waa ku meel gaadh, oo aluminium tuurista ayaa si otomaatig ah u baaba'aya markay sanduuqa ka baxaan. Si kastaba ha noqotee, waqtiga kala-bixinta aan habbooneyn ayaa badanaa sababa dildilaacyo kulul, gaar ahaan aluminium aluminium ah oo bir ah oo u nugul dillaacyada kulul ee walaacaas oo kale ah. Culeyska haraaga ah ee kujira aluminiumka kabka ayaa yareynaya aaladaha farsamo ee isku-darka wuxuuna saameyn ku yeelanayaa saxsanaanta mashiinka loo shubay. Feejignaanta haraaga ah ee aluminium tuurista waxaa lagu tirtiri karaa lifaaqa. Daawaha wuxuu leeyahay habsami u socodka kuleylka oo aan lahayn isbeddel waji ah inta lagu jiro habka qaboojinta. Ilaa iyo inta qaab dhismeedka ridaya loogu talagalay si macquul ah, culeyska haraaga ah ee aluminium shubka guud ahaan waa yar yahay.
(6) Neefsasho
Daawaha Aluminiumku waa fududahay in la nuugo gaaska, taas oo ah astaamaha ugu muhiimsan ee aluminium aluminium la tuuray. Haydarojiin ay soo saarto falcelinta udhaxeysa qaybaha aluminium dareeraha ah iyo kuwa aluminium ka sameysan iyo qoyaanka ku jira qarashka foornada, waxyaabaha dabiiciga ah ee waxyaabaha gubanaaya, iyo wasakhahaasi waxaa qaata dareeraha aluminiumka.
Heerkulka sare ee aluminiumku wuxuu dhalaalaa, hydrogen badan ayaa nuugaya. Marka la joogo 700 ° C, isku-milmika hydrogen-ka ee 100g aluminium ah waa 0.5 illaa 0.9. Marka heerkulku kaco ilaa 850 ° C, isku milmika hydrogen wuxuu kordhayaa 2 ilaa 3 jeer. Marka nijaasta biraha alkali ay ku jiraan, isku dhalaalka hydrogen ee aluminium la shubay ayaa si weyn kor loogu qaaday.
Marka lagu daro neefsashada aluminiumka aluminiumka ah inta lagu jiro dhalaalinta, waxay kaloo soo saartaa neefsashada marka ay ku shubaneyso caaryada. Birta dareeraha ah ee geleysa caaryada ayaa ku yaraata heerkulka, dareeraha gaaska ayaa yaraada, gaaska saa'id ahna waa la soo dejiyaa, waxaana jira qayb ka mid ah gaaska oo aan ka baxsan karin. Waxaa loo daayay sameynta daloolada si ay u sameyso daloolo, kuwaas oo badanaa loo yaqaan "pinholes". Gaaska mararka qaarkood wuxuu isku daraa godka yaraanshaha, gaaskuna wuxuu kuleel galaa aluminiumka la shubay wuxuu kusii nagaanayaa godka yaraanshaha. Haddii cadaadiska ka dhashay kuleylka ee goobooyinku ballaaran yihiin, dusha sare ee daloolada waa siman yihiin waxaana ku yaal daaha dhalaalaya hareeraha godadka; haddii cadaadiska ay dhaliyeen goobooyinku ay yar yihiin, dusha sare ee daloolada ayaa laalaabmay, taas oo u eg "cagaha lugaha", oo waxaa jira godad soo yaraanaya oo ku dhow kormeerka. Astaamaha.
Marka ay sare u kacdo waxa ku jira argon ee ku jira dareeraha daawaha ee aluminiumka la tuuro, ayaa waxaa sii kordhaya cirbadaha badan ee lagu soo saarayo ridaha. Pinholes-ka ku jira aluminium tuurista oo keliya ma yareynayso cidhiidhiga hawada iyo u adkaysiga daxalka ee kabka, laakiin sidoo kale waxay yareyneysaa astaamaha farsamo ee isku-darka. Si loo helo tuurista aluminium ee aan lahayn ama aan ka yareyn daloolada, furaha ayaa ku jira xaaladaha dhalaalida. Haddii wakiil dabool leh lagu daro ilaalinta inta lagu jiro dhalaalinta, qadarka neefsashada gaaska ee aaladda ayaa si weyn loo dhimay. Sifeynta aluminiumka la shubay ayaa si wax ku ool ah u xakameyn kara maaddada hydrogen ee ku jirta aluminiumka la shubay. Habka loo shubay ee adeegsada ciidda, dhoobada iyo qalabka kale ee kaabayaasha ah si loo sameeyo caaryo waxaa loo yaqaan "cast cast". Qalabka wasakhda ciidda waxaa si wada jir ah loogu yeeraa qalabka wax mideeya. Qaab-dhismeedka ciidda ee codsiyada biraha aan birta ahayn waxaa laga sameeyaa ciid, dhoobo ama wax kale oo wax ku dhejiya iyo biyo.
Nidaamka sameynta aluminium tuurista ayaa ah geedi socodka isdhexgalka birta iyo caaryada. Ka dib markii dareeraha aluminium ee aluminiumka lagu durayo caaryada, kuleylka waxaa loo wareejiyaa caaryada, iyo caaryada ciidda waxaa lagu soo rogaa saameynta kuleylka, farsamada, iyo kiimikada ee biraha dareeraha ah. Sidaa darteed, si loo helo tuuryo tayo sare leh, marka lagu daro si adag u hanashada geeddi-socodka dhalaalaya, sidoo kale waxaa lagama maarmaan ah in si sax ah loo naqshadeeyo caaryada (udub dhexaadka) saamiga ciidda, moodelinta iyo geeddi-socodka daadinta.
3. Tuurista Qaab Birta ah
1. Hordhac iyo habka farsamada
Tuurista caaryada birta waxaa sidoo kale loo yaqaannaa shubista caaryada adag ama shubista caaryada joogtada ah. Waa hab lagu shubo aluminiumka la dhalaalay ee lagu shubay caaryada birta ah si loo helo kabka. Inta badan aluminium aluminium tuurista caaryada waxay isticmaashaa diraha birta, laakiin sidoo kale ubucda ciidda ama diirkja qolofka. Habka, marka la barbar dhigo tuurista cadaadiska, aluminium caaryada birta ah waxay leedahay nolol adeeg dheer.
2. Faa'iidooyinka ridaya
(1) Faa'iidooyinka
Caaryada birtu waxay leedahay xawaare dhaqso badan oo qaboojin ah iyo qaab dhismeedka cufan ee ridaya, kaas oo lagu xoojin karo daaweynta kuleylka, astaamaheeda farsamo ayaa qiyaastii 15% ka sarreeya kan loo tuurayo ciidda. Tuurista caaryada birta ah, tayada wax loo shubay waa mid xasilloon, qallafsanaanta dusha sare ayaa ka wanaagsan roodhida ciidda, heerka xaddiga macdanta qashinka ayaa hooseysa. Xaaladaha shaqadu way fiican yihiin, waxsoosaarkuna waa sarreeyaa, shaqaaluhuna way fududahay in si fiican loo barto.
(2) Faa’iido daro
Nooca biraha wuxuu leeyahay hawo kululeyn ballaaran iyo karti xumo buuxinta. Nooca biraha laftiisu ma laha marin hawo. Tallaabooyinka u dhigma waa in loo qaadaa si waxtar leh u dhammaystira. Caaryada biraha ma leh dib u gurasho waana fududahay in la dillaaco oo qaab yeesho inta lagu gudajiro adkeynta.
3. Cilladaha guud iyo ka hortagga tuurista birta
(1) god-god
Tallaabooyinka looga hortagayo godadka godadka: Waxaa si adag loo mamnuucay in la isticmaalo walxaha aluminiumka aluminiumka lagu tuuray ee wasakhaysan, walxaha wasakhaysan xeryahooda dabiiciga ah oo si xun u oksaydh ah oo la shiiday xakameeyo habka dhalaalka, xoojinta kala-soocidda iyo sifaynta; xakamee dhumucda dahaadhka nooca birta, aad u qaro weyn ayaa fududahay in la soo saaro godad goos goos ah; Heerkulka caaryadu waa inuusan aad u sarreyn, qaad tallaabooyinka qaboojinta ee qaybaha darbiga qaro weyn ee jilayaasha, sida naxaasta ama biyo-gelinta, iwm. markaad isticmaaleyso wasakhda ciidda, si adag u xakamee qoyaanka iskuna day inaad isticmaasho diirkja qalalan.
(2) Stoma
Tallaabooyinka looga hortagayo daloolada: wax ka beddel nidaamka daadinta iyo soo kicinta aan macquul ahayn si dareeraha qulqulaya looga dhigo mid deggan oo looga fogaado gaaska inuu lug ku yeesho; caaryada iyo udub-dhexaadka waa in la diiriyaa ka hor, ka dibna la rinjiyeeyaa, waana in si fiican loo qalajiyaa ka hor intaan la isticmaalin; naqshadeeyaan caaryada Tallaabooyinka qiiqa oo ku filan waa in lagu tixgeliyaa xudunta.
(3) Oxidation iyo slag ka mid noqoshada
Tallaabooyinka looga hortagayo oksaydhka iyo ka-mid noqoshada slag: si adag u xakamee geedi socodka dhalaalinta, dhalaalida dhakhsaha badan, yareynta oksaydhka, oo si fiican uga saar dhirta. A1- Mg alloy waa in lagu dhalaaliyaa wakiilka daboolaya; foornada iyo qalabku waa inay ahaadaan kuwo nadiif ah, oo aan lahayn oksaydh, waana in la sii kululeeyaa, dahaadhkuna waa in la qalajiyaa si loo isticmaalo ka dib markii uu gaabis sameeyo;
Nidaamka wax lagu shubayo ee loogu talagalay waa inuu lahaadaa qulqulo xasiloon, keydsan kara iyo karti-u-dhicid; nidaamka qulqulaya qulqulaya ayaa loo isticmaalaa in lagu xasiliyo qulqulka dareeraha iyada oo aan lahayn qiiqa labaad; daahan la xushay waa inuu lahaadaa adhesion xoog leh, oo ma kala bixin doono inta lagu gudajiro hawsha shubista oo wuxuu galayaa dahaarka si loo sameeyo Slag.
(4) Dildilaaca kuleylka
Tallaabooyinka looga hortagayo dildilaaca kuleylka: Kuleylka maxalliga ah waa in laga fogaadaa nidaamka shubaasha dhabta ah si loo yareeyo buuqa gudaha; u janjeedha caaryada iyo udub-dhexaadka waa inay ka sarreeyaan 2 °, kicinta soo shubashadana waa la jiidi karaa si loo furo caaryada marka ay adkaato, iyo udub dhexaadka ciidda waa la isticmaali karaa haddii loo baahdo Beddel xudunta biraha; xakamee dhumucda dusha si looga dhigo heerka qaboojinta qayb kasta oo ka mid ah ridayadu mid joogto ah; Xullo heerkulka caaryada ee ku habboon dhumucda shubista; sifeeyo qaab-dhismeedka daawaha si loo hagaajiyo awoodda qabashada kulul; hagaajinta qaab dhismeedka tuubada si looga takhaluso geesaha fiiqan iyo is-beddellada dhumucda darbiga, Yaree u janjeera dilitaanka kulul
(5) Dabacsan
Tallaabooyinka looga hortagayo dabaysha: dejinta macquulka ah ee macquulka ah si loo hubiyo xoojinta iyo awoodda quudinta; si habboon hoos ugu dhig heerkulka shaqada ee caaryada birta ah; xakameynaya dhumucda lakabka oo yareynaya dhumucda darbiga qaro weyn; hagaaji heerka qaboojinta ee qayb kasta oo ka mid ah caaryada birta ah si loo sameeyo Darbiga qaro weyn ee loo shubay wuxuu leeyahay awood dhiirrigelin oo weyn; si ku habboon u yareeyn heerkulka biraha ku shubaya.
Bogag laxiriira: Casting Aluminium
Maqaallo la xidhiidha:
- Saamaynta Birta Oxide ee Tayada Taagista Dahaarka Daawaha Aluminium
- Codsiga Qalabka Aluminium ee Aluminium ee Baabuurta
Fadlan hayso isha iyo cinwaanka maqaalkan si dib loogu daabaco:Faa'iidooyinka iyo Faa'iido-darrada Geeddi-socodka Daarista Aluminium
Minghe Shirkadda Die Casting waxaa ka go'an in ay soosaaraan oo ay bixiyaan Qaybo ka ridaya tayo iyo waxqabad sare (biraha qaybo ka ridaya dhiman kala duwan inta badan ka mid yihiin Khafiifa-Wall dhinta ridaya,Hot ridaya die Cast,Kursiga Qabow Die Casting), Adeeg Wareeg ah (Adeegga Tartanka Dhimashada,Qalabka Mashiinka,Samaynta Furka, Daaweynta Dusha sare) .Caadi kasta oo Aluminium ah shubitaan, magnesium ama Zamak / zinc shubida iyo shuruudaha kale ee shubanka ayaa lagu soo dhaweynayaa inaad nala soo xiriirto.
Iyada oo ay gacanta ku hayaan ISO9001 iyo TS 16949, dhammaan geeddi-socodyada waxaa lagu fuliyaa iyada oo loo marayo boqollaal mashiinno shub ah oo dhimanaya, mashiinnada 5-dhidibka, iyo tas-hiilaadka kale, oo ka bilaabma qarxiyayaal ilaa mashiinnada dharka lagu nadiifiyo ee Ultra Sonic.Minghe ma ahan oo keliya qalab casri ah laakiin sidoo kale waxay leedahay xirfadle koox injineero khibrad leh, wadayaal iyo kormeerayaal si niyada macaamiisha ay u noqoto mid run ah.
Soo saaraha qandaraasle ee shubka dhinta. Awoodda waxaa ka mid ah qaybaha qabow ee aluminium ee qaybaha shubista laga bilaabo 0.15 lbs. illaa 6 rodol, isbeddel deg deg ah oo la dejiyay, iyo qalabaynta. Adeegyada qiimaha lagu daro waxaa ka mid ah sifaynta, gariirka, qashin-qubka, xabbadda toogashada, ranjiyeynta, dahaadhka, dahaadhka, isku-ururinta, iyo qalabaynta. Qalabka lala shaqeeyay waxaa ka mid ah alloysyada sida 360, 380, 383, iyo 413.
Zinc wuxuu u dhintaa caawinta naqshadeynta / adeegyada injineernimada isku mar. Soo saaraha gaarka ah ee saxda saxda ah ee looxyada. Daarayaasha yar-yar, cast-yada u dhinta cadaadiska sare, jilayaasha caaryada badan-slide, shubka caaryada caadiga ah, cutubka dhinta iyo kuwa madaxa-bannaan ee loo dhinto iyo daloolka dahaarka saanlan ayaa la soo saari karaa. Jilayaasha waxaa lagu soo saari karaa dherer iyo ballac ilaa 24 gudaha. +/- 0.0005 gudaha. Dulqaad.
ISO 9001: soo saaraha shahaadada leh ee loo yaqaan 'cast cast magnesium', Awoodaha waxaa ka mid ah dhimista cadaadiska sare ee magnesium oo loo ridayo ilaa 2015 ton qol kulul & 200 ton oo qol qabow ah, naqshadeynta qalabka, nadiifinta, wax u sameynta, mashiinada, budada & dareeraha rinjiyeynta, QA buuxda oo leh awooda CMM , ururinta, baakadaha & gaarsiinta.
ITAF16949 la xaqiijiyay. Adeeg Dheeraad Dheeraad ah Ayaa Kujira maalgelinta maalgelinta,ciida ciid,Dabaaldeg Shaqo, Casting Foam Fost,Khadka Centrifugal,Dabka Vacuum Casting,Qaab Joogtada ah, Awoodda waxaa ka mid ah EDI, kaalmada injineernimada, qaabeynta adag iyo ka shaqeynta heerka labaad.
Warshadaha Kabka Qaybaha Daraasada Kiiska ee loogu talagalay: Gawaarida, Baaskiiladaha, Diyaaradaha, Qalabka muusikada, Biyaha, Qalabka indhaha, Dareemayaasha, Moodooyinka, Aaladaha elektarooniga ah, Xiritaanka, Saacadaha, Mashiinnada, Mashiinnada, Qalabka guryaha, Dahabka, Jigs, Telecom, Laydhka, Qalabka Caafimaadka, Qalabka Sawirka, Robotyo, farshaxanno, qalabka codka, Qalabka isboortiga, Qalabaynta, Caruurta iyo waxyaabo kale oo badan.
Maxaan kaa caawin karnaa inaad sameyso marka xigta?
Tag bogga hore ee loogu talagalay Shiinaha dhinta Casting
→Qeybaha kabkaOgow waxaan soo qabanay.
Tips Tilmaamaha Halaasiga ah ee Ku Saabsan Adeegyada Cast Cast
By Soo saaraha Minghe Die Casting | Qeybaha: Maqaallo waxtar leh |Waxyaabaha Tags: Casting Aluminium, Tuurista Zinc, Ridaya Magnesium, Qalitaanka Titanium, Qalabka birta ee birta, Naxaas naxaas ah,Raxaama Naxaas,Video Tuuraya,Taariikhda Shirkadda,Calaamadda Aluminum Die Casting | Faallooyinka Off