Marka hore, talaabooyinka xulashada mashiinka ridaya dhinta
- 1) Xisaabi xuduudaha farsamo iyo wax soo saar ee mashiinka wax lagu shubo ee dhinta iyadoo la raacayo shuruudaha farsamo, shuruudaha adeegsiga iyo qeexida geedi socodka dhimashada-tuurista kabka, marka horena dooro qaabka ku haboon.
- 2) Marka loo eego fikradda hordhaca ah ee caaryada dhinta-qaadista (caaryada) xuduudaha farsamo iyo shuruudaha nidaamka, xisaabi cabirka geedi-socodka shubanka iyo cabirka caaryada dhinta-qaadista (caaryada) cabirka, oo xulo qaabka ku habboon.
- 3) Qiimee waxqabadka shaqada iyo saameynta dhaqaale ee mashiinka wax lagu rido, oo ay kujiraan dhalidda, heerka gudbinta, waxsoosaarka, iyo xasiloonida howlgalka, kalsoonida, iyo amniga.
Second, habka xulashada ee mashiinka shubay dhinta
1) Soosaarka dhabta ah, doorashada mashiinka shubka dhinta wuxuu inta badan ku saleysan yahay nooca dawalada dhinta-tuurista, cabirka dusha iyo culeyska shubka si loo go'aamiyo isticmaalka qolka-kulul ama mashiinada qabow-qolka qabow. Wixii looxyada daawaha zinc iyo shubka dahaarka magnesium yar yar, qolka kulul mashiinada ridaya inta badan waa la isticmaalaa. Wixii daawaha aluminium, castings daawaha alloy iyo castings daawaha weyn ee magnesium, qolka qabow mashiinada ridaya dhinta yihiin doorashada ugu weyn. Qolka qabow ee toosan mashiinka ridaya ayaa ku haboon tuurista leh qaababka radial-dhexe iyo qaabeeyayaasha isla mar ahaantaana leh shuruudaha furitaanka orod dhexe.
2) Marka loo eego maaddada, cabbirka dulucda, celceliska dhumucda gidaarka, iyo miisaanka saafiga ah ee qaybaha dhinta-ridaya, xulo qaabka iyo tilmaamaha mashiinka wax lagu shubay. Xuduudaha habka dhabta ah sida qiimaha qufulka (caaryada) xoogga, xaddiga ku shubashada markasta, iyo buuxinta qolka duritaanka waxaa lagu heli karaa xisaabinta iyadoo saldhig u ah xulashada qaabka.
3) Cabirka caaryada dhinta-shubka (caaryada) waa inay u dhigantaa xajmiga u dhigma ee caaryada (caaryada) lagu rakibay mashiinka ridaya. Qiyaasaha ugu weyni waa dhumucda caaryada dhinta-tuurista (caaryada) iyo masaafada u dhexeysa dusha kala-baxa caaryada (caaryada). Waa inuu buuxiyaa shuruudaha xuduudaha aasaasiga ah ee mashiinka wax lagu rido:
- Dhumucda H ee caaryada dhinta-qaadista (caaryada) waa inaysan ka yareynin caaryada ugu yar (caaryada) dhumucda lagu sheegay buugga mashiinka, mana ka weynaan karto caaryada ugu badan ee caarada ah (caaryada) ee la bixiyo, H dejinta waa inay ahaataa buuxiyaan shuruudaha soo socda; Hmin + 10mm≤ H set ≤ Hmax-10mm; Halka H lagu dhigay - dhumucda qaabka loo qaabeeyey (caaryada) (mm) ;; Hmin - dhumucda ugu yar ee caaryada la siiyay (caaryada) dhimashada - baahinta qaybta, taas oo ah, "dhumucda caaryada" (mm) ;; Hmax - Dhumucda ugu sarreysa ee caaryada (caaryada) ee uu bixiyo mashiinka dhinta-tuurista, taasi waa, "dhumucda caaryada" (mm).
- MachineKa dib markii mashiinka-shubista uu furo caaryada (caaryada), istaroogga (L) ee mashiinka gawaarida gawaarida gawaarida (caaryada) saxanka kursiga, taas oo ah, masaafada udhaxeysa caaryada dhinta (caaryada) iyo dusha kala taga, waa inuu ka weynaadaa ama u dhigmaa masaafada ugu yar ee daweyn kara.
L≥L qaado
Jaantuska 1 wuxuu muujinayaa masaafada ugu yar ee caaryada dhinta-tuurista (caaryada) oo ay riixday usha riixistu si ay u soo saarto ridaha.
L wuxuu qaataa coreL core + L gabal + K; Qaaciddada, K guud ahaan wuxuu qaataa 10mm.
3. Tusaalooyinka qaabka xulashada mashiinka ridaya dhinta, Tusaale ahaan, ridaya qaab sanduuqa waa la yaqaan, sida ku cad Jaantuska 2. Kuwa soo socda ayaa ah falanqeyn xul ah oo ku saleysan xuduudaha farsamo ee mashiinka tuurista dhinta ee jiifka jiifa. Lijin Mashiinka Factory Co., Ltd. Qalabka xaalad aasaasiga ah waa aluminium daawaha; cabirka guud (dherer × width × height) waa 280mm × 180mm × 80mm; celceliska dhumucda derbiga waa 3 mm; miisaanka saafiga ah ee ridaya waa 1240g
1. Xisaabi aagga la saadaaliyay ee kabka
A1=280mm×180mm=50400mm2
Nidaamka orodka A2 = (0.15 ~ 0.30), 0.21 ee A2
Then A2=0.21×50400mm2=10584mm2
Waxyaabaha haraaga ah (keeg) A3 = πd2 / 4, dhexroorka d qolka xulashada cadaadiska waa φ70mm (taas oo ah, dhexroorka feerku waa -70), ka dibna A3 = 3847mm2
Nidaamka sii-deynta A4 = (0.1 ~ 0.2), haddii A1 doorto 0.12
A4=A1*0.12=6048mm2
Wadarta aagga la saadaaliyay:
A=A1+A2+A3+A4=50400mm2+10584mm2+3847mm2+6048mm2=70879mm2
2. Xisaabi xoogga qulqulaya, qufulka xoogga, oo xulo nooca bilowga ah
(1) Haddii ridayadu leedahay shuruudo guud oo keliya isla markaana ka tirsan tahay qaybaha caadiga ah, xulo kor u qaadista cadaadiska pbz = 40N / mm2 (MPa), F ballaarinta = 40N / mm2 × 70879mm2 = 2835160N, F qufulka = F ballaarinta / K, qaado K = 0.85 F quful = 2835160N / 0.
85 = 3335482N = 3335.482kn
Moodalka leh quful quful ah 4000kn waa la dooran karaa, qaabka DCC400 waxaa loo xushay mashiinka xoogga.
2 mm2 (MPa) F ballaarinta = 70N / mm2 × 70879mm2
= 4961530N, F qufulka = F ballaarinta / K, qaado K = 0.85 F qufulka
= 4961530N / 0.85 = 5837094N = 5837.094 kn
Moodhalka leh quful quful leh oo ah 6300kn waa la dooran karaa, qaabka DCC630 ayaa loo xushay mashiinka xoogga.
3. Xisaabi culeyska dareeraha daawaha ah ee la shubay
Miisaanka saafiga ah ee loo shubay waa G1 = 1240g; jadwalka wuxuu muujinayaa in cufnaanta dareeraha ee aluminium-ka y = 2.5g / cm3. Nidaamka muruqyada 'G2' wuxuu dejiyaa celceliska qoto dheer (dhumucda) muruqyada inuu noqdo 7mm (0.7cm)
G2=V2 ρ=A2×0.7×2.5=186g
Haraaga walxaha (keeg) G3 Calan dhumucda walxaha haraaga noqo 30mm (3cm) G3 = V3
= A3 × 3 × 2.5 = 288.5g
Nidaamka qulqulka G4 wuxuu leeyahay qoto dheer jeexdin jeexjeexan oo ah 6mm (0.6cm)
G4 = V4 ρ = A4 × 0.6 × 2.5 = 90.8g wadarta culeyska biraha la shubay
G=G1+G2+G3+G4 =1.81kg
4. Xisaabi buuxinta qolka cadaadiska
(1) Marka la xusho DCC400, qadarka daadinta ee dhexroorka feerka φ70 waa 3.6kg. Buuxnaanta φ = 1.81 / 2.6 × 100% = 50.3% Badanaa buuxintu waxay kujirtaa inta udhaxeysa 40% ilaa 75%. Xulashada kore ee DCC400 waxay buuxineysaa shuruudaha.
(2) Marka la xusho DCC630, qadarka daadinta ee dhexroorka feerka φ70 waa 4.3kg, iyo darajada buuxintu waa φ = 1.81 / 4.3 × 100% = 42.1%. DCC630 sidoo kale waxay buuxisaa shuruudaha.
5. Xiriirka ka dhexeeya caaryada dhinta-tuurista (caaryada) iyo baaxadda caaryada mashiinka ku sii xirmaya
Mashiinka sii kordhaya ee mashiinka waxaa laga helaa qaababka DCC400 iyo DCC630, khafiifinta caaryada, dhumucda caaryada, istaroogga saxanka la dhaqaajin karo, cabirka gudaha ee u dhexeeya dhejiska dhejiska, iyo xuduudaha farsamada, kuwaas oo loogu talagalay xisaabinta. In cabirka u dhigma ee caaryada dhinta-tuurista (caaryadu) ay la kulmi karto shuruudaha.
6. Si loo xisaabiyo tamarta cirbadeynta
isticmaal cadaadiska ugu sarreeya ee birta ah ee nidaamka duritaanka iyo jaantuska xiriirka xiriirka P-Q2 si loo falanqeeyo, loona xisaabiyo in waxqabadka duritaanka ee mashiinka-tuurista dhinta ee la xushay ay buuxin karto shuruudaha tamarta loo baahan yahay. Ka dib markii la xisaabiyo xuduudaha kala duwan ee mashiinka, nooca mashiinka dhinta-ridaya ayaa aragti ahaan lagu go'aamin karaa.
Fadlan hayso isha iyo cinwaanka maqaalkan si dib loogu daabaco: Xulista Mashiinka Mashiinka Dhimashada
Minghe Shirkadda Die Casting waxaa ka go'an in ay soosaaraan oo ay bixiyaan Qaybo ka ridaya tayo iyo waxqabad sare (biraha qaybo ka ridaya dhiman kala duwan inta badan ka mid yihiin Khafiifa-Wall dhinta ridaya,Hot ridaya die Cast,Kursiga Qabow Die Casting), Adeeg Wareeg ah (Adeegga Tartanka Dhimashada,Qalabka Mashiinka,Samaynta Furka, Daaweynta Dusha sare) .Caadi kasta oo Aluminium ah shubitaan, magnesium ama Zamak / zinc shubida iyo shuruudaha kale ee shubanka ayaa lagu soo dhaweynayaa inaad nala soo xiriirto.
Iyada oo ay gacanta ku hayaan ISO9001 iyo TS 16949, dhammaan geeddi-socodyada waxaa lagu fuliyaa iyada oo loo marayo boqollaal mashiinno shub ah oo dhimanaya, mashiinnada 5-dhidibka, iyo tas-hiilaadka kale, oo ka bilaabma qarxiyayaal ilaa mashiinnada dharka lagu nadiifiyo ee Ultra Sonic.Minghe ma ahan oo keliya qalab casri ah laakiin sidoo kale waxay leedahay xirfadle koox injineero khibrad leh, wadayaal iyo kormeerayaal si niyada macaamiisha ay u noqoto mid run ah.
Soo saaraha qandaraasle ee shubka dhinta. Awoodda waxaa ka mid ah qaybaha qabow ee aluminium ee qaybaha shubista laga bilaabo 0.15 lbs. illaa 6 rodol, isbeddel deg deg ah oo la dejiyay, iyo qalabaynta. Adeegyada qiimaha lagu daro waxaa ka mid ah sifaynta, gariirka, qashin-qubka, xabbadda toogashada, ranjiyeynta, dahaadhka, dahaadhka, isku-ururinta, iyo qalabaynta. Qalabka lala shaqeeyay waxaa ka mid ah alloysyada sida 360, 380, 383, iyo 413.
Zinc wuxuu u dhintaa caawinta naqshadeynta / adeegyada injineernimada isku mar. Soo saaraha gaarka ah ee saxda saxda ah ee looxyada. Daarayaasha yar-yar, cast-yada u dhinta cadaadiska sare, jilayaasha caaryada badan-slide, shubka caaryada caadiga ah, cutubka dhinta iyo kuwa madaxa-bannaan ee loo dhinto iyo daloolka dahaarka saanlan ayaa la soo saari karaa. Jilayaasha waxaa lagu soo saari karaa dherer iyo ballac ilaa 24 gudaha. +/- 0.0005 gudaha. Dulqaad.
ISO 9001: soo saaraha shahaadada leh ee loo yaqaan 'cast cast magnesium', Awoodaha waxaa ka mid ah dhimista cadaadiska sare ee magnesium oo loo ridayo ilaa 2015 ton qol kulul & 200 ton oo qol qabow ah, naqshadeynta qalabka, nadiifinta, wax u sameynta, mashiinada, budada & dareeraha rinjiyeynta, QA buuxda oo leh awooda CMM , ururinta, baakadaha & gaarsiinta.
ITAF16949 la xaqiijiyay. Adeeg Dheeraad Dheeraad ah Ayaa Kujira maalgelinta maalgelinta,ciida ciid,Dabaaldeg Shaqo, Casting Foam Fost,Khadka Centrifugal,Dabka Vacuum Casting,Qaab Joogtada ah, Awoodda waxaa ka mid ah EDI, kaalmada injineernimada, qaabeynta adag iyo ka shaqeynta heerka labaad.
Warshadaha Kabka Qaybaha Daraasada Kiiska ee loogu talagalay: Gawaarida, Baaskiiladaha, Diyaaradaha, Qalabka muusikada, Biyaha, Qalabka indhaha, Dareemayaasha, Moodooyinka, Aaladaha elektarooniga ah, Xiritaanka, Saacadaha, Mashiinnada, Mashiinnada, Qalabka guryaha, Dahabka, Jigs, Telecom, Laydhka, Qalabka Caafimaadka, Qalabka Sawirka, Robotyo, farshaxanno, qalabka codka, Qalabka isboortiga, Qalabaynta, Caruurta iyo waxyaabo kale oo badan.
Maxaan kaa caawin karnaa inaad sameyso marka xigta?
Tag bogga hore ee loogu talagalay Shiinaha dhinta Casting
→Qeybaha kabkaOgow waxaan soo qabanay.
Tips Tilmaamaha Halaasiga ah ee Ku Saabsan Adeegyada Cast Cast
By Soo saaraha Minghe Die Casting | Qeybaha: Maqaallo waxtar leh |Waxyaabaha Tags: Casting Aluminium, Tuurista Zinc, Ridaya Magnesium, Qalitaanka Titanium, Qalabka birta ee birta, Naxaas naxaas ah,Raxaama Naxaas,Video Tuuraya,Taariikhda Shirkadda,Calaamadda Aluminum Die Casting | Faallooyinka Off