Habka Iyo Codsiga Dahaarka Moldashiinka Mashiinka Caanka ah ee Sand-Coated
Muxuu Yahay Sand-Dahaarka Birta U Qaadaya
Mashiinka birta ah ee loo yaqaan 'cast steel sand-coated casting' waa geedi socod loo shubay oo lakab khafiif ah oo ciid ah lagu daboolayo daloolka hoose ee caaryada birta ah (oo loo yaqaan birta) Sababtoo ah lakabka dahaadhka ciidda ayaa ah mid dhuuban (4 ~ 8mm), waa macquul macquul ahaan in la isticmaalo qalab qaali ah oo tayo sare leh. Natiijo ahaan, tayada jilayaasha ayaa si weyn loo hagaajiyay qashinkana si weyn ayaa loo yareeyay; adadag darrada birta ku dahaadhan birta caaryada Aad u wanaagsan, oo markaa si weyn u wanaajinaysa saxnaanta cabbirka iyo isukeenista rida.
Jarmalka, Midowgii Soofiyeeti hore iyo dalal kale waxay bilaabeen inay adeegsadaan shubka birta ku dahaadhan birta wax soo saarka shubka qiyaastii sanadihii 1960-meeyadii, inta badan soosaarka crankshafts birta ductile, xargaha kala jejebinta, saxannada biriga, qalabka silsiladda, bambooyin bambooyin, taangiyada hareeraha iyo saldhigyada mootada , iwm Noocyada loo tuuro. Cilmi-baarista dalabka Shiinaha ee ku saabsan shubka caaryada ku duuban caaryada birta waxay bilaabatay horraantii 1970-naadkii. By 1979, Zhejiang makaanik iyo Machadka Naqshadeynta Korantada iyo Yongkang cagaf Warshadda ayaa iska kaashaday in ay adeegsadaan howshan markii ugu horreysay wax soo saarka shubista tirada badan ee meelaha faaruqinta ah ee S195. Isla mar ahaantaana, qiimeynta waxqabadka ee birta qulqulka birta ee ay soo saartay geeddi-socodkan ayaa la dhammaystiray, marka la eego awoodda daalka (isbarbardhiga daalka xaddidaadda daalka σ-1), xoogga jabka (isbarbardhigga qiimaha marinka thKth iyo isbarbardhigga adkaanta jabka K1C ) iyo nolosha adeegga (Isbarbar dhigga imtixaanka dulqaadka ee kursiga keydka 10000h), iwm, marka la barbar dhigo crankshaft ee tuurista ciidda, way ka wanaagsan tahay rida ciidda. 10-ka sano ee soo socda, hawsha si isdaba-joog ah ayaa loogu hagaajiyay arjiga. Horraantii 1990-meeyadii, toddobo shirkadood ayaa hirgeliyay howsha, gaar ahaan hannaanka loo shubay birta ee birta ku dahaadhan hal-dhululubo iyo afar-dhululubo goos goos ah. Guul weyn. Shirkadaha matala mudadan waa Yongkang cagaf Factory, Shangyu Power Makiinado Warshad, Wangdu Crankshaft iyo Isku xidhka Warshada Rod, Wanbei Crankshaft Factory, Jinhua Internal Combustion Engine Parts Factory, Changzhou Diesel Engine Factory, iwm. Sanadkii 1991, Gudiga Qorshaynta Gobolka ayaa ansixiyay birta caaryadu waxay u shubtay ciid-dahaarka leh oo ah mashruuc muhiim u ah dhiirrigelinta tikniyoolajiyadda ee "Qorshaha Shanta Sano ee Siddeedaad" ee dalka, wuxuuna ka dhigay Zhejiang makaanik iyo Machadka Naqshadeynta Korantada inuu noqdo qeybta taageerada farsamo ee mashruuca. Tani waa horumar weyn oo dhanka tiknoolajiyada tuurista ciidda ah ee caaryada birta ah ee dalkayga. Horumarku wuxuu door weyn ka ciyaaray kobcinta. Ka dib markii machadkeennu uu guda galay mashruuca dhiirrigelinta, 5ta illaa 6da sano ee soo socda, dhibaatooyin taxane ah oo ah birta dahaarka leh ee birta loo soo tuuray ee wax soo saarka ballaaran ayaa asal ahaan la xaliyay.
Inta badan:
- ①Waxaa la naqshadeeyay oo la dhammaystiray mashiinka wax lagu duubo ee ciiddu ku dahaadhan tahay, kaas oo xalliyay dhibaatada muddada dheer taagnayd ee ka-beddelidda iyo beddelidda xabbadaha muhiimka ah;
- Line Khadadka wax soo saarka shubista ee dhoobada cufan ee nooca birta ah ayaa la dhammaystiray oo la jaangooyay, iyo soosaarka asalka ah ee fudud ee wax soo saarka dhoobada ciidda lagu soo rogay ayaa la hagaajiyay laguna dabaqay shirkadaha sida Shanghai Nodular Iron Plant;
- Codsiga dhoobada birta ah ee cufan-dahaarka leh ayaa lagu balaariyay qaar ka mid ah shubanka oo leh geedi socod ku shubista dhib badan, sida crankshafts lix-dhululubo ah iyo crankshafts saddex-dhululubo ah;
- Ku soo bandhigida carrada dahaarka leh soosaarka birta dahaarka leh ee birta lagu xirayo, iyadoo si weyn kor loogu qaadayo tayada wax-u-beddelidda ciidda lagu dahaadhay;
- ⑤Nashqad-samaynta birta qaab-dhismeedka loo shubay ciidda caaryada birta ah ayaa la sii dheellitiray, heerka naqshaduna sidoo kale si weyn ayaa loo hagaajiyey. Barnaamijka jilitaanka kumbuyuutarka ee habka shubista caaryada ee caaryada birta ah iyo softiweerka naqshadeynta kumbuyuutarka ee hannaanka loo shubay caaryada caaryada birta ah ayaa la soo saaray.
Waqtigan xaadirka ah, ku dhowaad boqol shirkadood oo waddanka oo dhan ah ayaa dalbaday habka birta ah ee loo duubay birta birta ah si ay u soo saaraan in ka badan 30 nooc oo shub ah sida crankshafts birta ductile, camshafts, fallaadhihii dheelitirka, meydadka waalka cadaadiska u adkaysta, silsiladaha silsiladda, iyo xirashada u adkaysta saxannada qalabka. Wax soo saarka sanadlaha ah waxaa lagu qiyaasaa inuu yahay shubmo. Qiyaastii 10 × 104t. Shirkadaha caadiga ah waxaa ka mid ah Shanghai Automobile Foundry General Ductile Iron Factory, Shenyang No. 1 Crankshaft Factory, Guangxi Baikuang Group, Yixing Machinery General Factory, Shandong Jiuyang Group, Zhejiang Shuguang Crankshaft Factory, Benxi Tianyuan Crankshaft Factory, Baoding Film Machinery Factory, Shanxi Lung. , Hebei Xinji Crankshaft Factory, iwm. Si kastaba ha noqotee, shirkadahaani waxay leeyihiin habab kala duwan oo ay ku soo bandhigayaan habka: qaar baa ku aaminay machadkeena inuu naqshadeeyo ama dhiso, qaarna waxay ku daydeen oo ay iskiis u horumariyeen. Sidaa darteed, xooggooda hanashada birta qaab-dhismeedka shubidda ee caaryada birtu aad ayey u kala duwan tahay. Qaadashada kaliya heerka qashinka tuuraya caaryada birta ah ee dahaarka ah tusaale ahaan, shirkado badan oo haysta faham wanaagsan ayaa xasilin kara qiyaastii 3%, waxayna gaareen faa'iidooyin dhaqaale oo aad u wanaagsan. Si kastaba ha noqotee, waxaa sidoo kale jira shirkado yar oo caaryada birta ah ee qashinka lagu shubo qashinka ay gaarayaan ilaa 20%, taas oo si weyn uga soo horjeedda faa'iidooyinka dhaqaale ee hawshan. Sababta ayaa ah in shirkadahan aysan si buuxda u fahmin naqshadeynta iyo soo saarida waxyaabaha muhiimka u ah geedi socodka, isla markaana la dayacay maaraynta wax soo saarka.
Xalalka ugu muhiimsan ee naqshadeynta iyo wax soo saarka dhabta ah ee birta qaabka loo shubay ciidda dhoobada leh:
- Dhumucda derbiga birta iyo dhumucda lakabka bacaadka iyo isku darka labada waxay buuxin karaan shuruudaha kala duwan ee ku saabsan adkeynta iyo qaboojinta tuurista leh dhumucda derbiga ee kala duwan iyo qalabka kala duwan;
- Method Qaab dhismeedka daahan ciidda habboon iyo mid dhaqaale ee ku habboon si loo buuxiyo shuruudaha tuurista kala duwan ee tayada dusha sare iyo saxnaanta cabbirka;
- Halbeegyada waxqabadka Sida go'aaminta nidaamka qolqolka, nidaamka toogashada ciidda, nidaamka qiiqa, iwm;
- Xaqiijinta wax soosaarka tirada badan. Tusaale ahaan, qaabeynta iyo qaabka xariiqda wax soo saarka iyo martida ciidda daboolan iyo qalabka caawinta;
- Sameynta xeerarka nidaamka, sida qawaaniinta shubista, qaboojinta iyo furfurista, iyo sidoo kale hagaajinta halabuurka shayga.
Astaamaha Isweydaarsiga Heat ee Nooca Birta ah ee Tuurista Daboolaha
Ka dib marka biraha dareeraha ah lagu shubo caarada birta ee dahaarka leh ee birta lagu duubay, "shubista-ciidka-caaryada birta ah" waa nidaam is-weydaarsiga kuleylka oo aan degganeyn. Si loo fududeeyo dhibaatada, waxaa loo maleynayaa in ridayadu tahay mid xadidan; waxaana loo maleynayaa in qaybta heerkulka ee qayb kasta oo ka mid ah nidaamka loo qaybiyo khad toosan. Jaantuska 1 wuxuu muujinayaa qayb ka mid ah nidaamka. Sida iska cad, isla socodka kuleylka gaarka ah q wuxuu maraa qayb kasta oo nidaamka ka mid ah:
Laba shuruudood oo wareejinta kuleylka siday u kala horreeyaan oo matalaya xoojinta is-weydaarsiga kuleylka ee u dhexeeya ridaya iyo lakabka ciidda daboolan, iyo caaryada birta ah iyo lakabka ciidda daboolan. k1 waa saamiga u adkaysiga kuleylka ee ridaya ilaa caabbinta kuleylka ee daboolka ciidda; k2 waa saamiga u adkaysiga kuleylka ee nooca birta ilaa caabbinta kuleylka ee daboolka ciidda. Iyadoo la tixgelinayo isku darka k1 iyo k2, iyadoo la beddelayo dhumucda dusha sare ee ciidda, waxaa jira seddaxdan xaaladood ee kala-wareejinta kuleylka kala duwan ee u dhexeeya "ridaya-ciidda dahaarka-caaryada birta ah" ee run ahaantii dhici karta:
- Marka k≤1 iyo k2≤1, lakabka dusha sare ee ciiddu wuxuu ku dhex jiraa dhumucda caadiga ah, heerka qaboojinta ee ridaya ayaa sii kordheysa iyadoo dhumucda lakabka daaha ciiddu hoos u dhacayso.
- Markay dhumucda lakabka ciidda lagu dahaadhay ay dhaafto dhumuc cayiman, caaryada birtu wax saamayn ah kuma laha qaboojinta ridaha. Waqtigaan, waxay u dhigantaa ciida caadiga ah ee la tuurayo ama ridaha dhoobada. Maaddaama kuleylka kuleylka lakabka bacda leh uu aad uga yar yahay kan birta ah, shubku si tartiib ah ayuu u qaboobaa.
- HenMarka k ≧ 1 iyo k2 ≧ 1, dhumucda dusha ciidku aad ayuu u khafiifsan yahay, kaasoo u dhigma ka sameysma caaryada birta ah.
Sifooyinka sarrifka kuleylka ee kor ku xusan waxaa lagu xaqiijiyay tijaabooyin. Marka dhumucda lakabka bacda ee crankshaft (CTЦ-14) birta nooca-birta loo shubay si tartiib tartiib ah isu beddelo 4 ilaa 32 mm, qadarka sibidhka ee dhismaha crankshaft ayaa si isdaba joog ah loo dhimay, iyo xaddiga pearlite iyo The xaddiga ferrite ayaa sii kordhaya. Marka dhumucda lakabka ciidda lagu dahaadhay ay ka yar tahay 4mm, xoogga qaboojinta ee ridaya wuxuu la mid yahay kan birta ah (rinjiga qaro weyn); marka lakabka ciidda lagu dahaadhay uu ka weyn yahay 32mm, xoogga qaboojinta wuxuu u dhigmaa kan ridaya ciidda cusbi ee caadiga ah.
Marka loo isticmaalo kabka birta ah ee ku dahaadhan birta soosaarka noocyo kala duwan oo jilitaan ah, waa iyada oo loo marayo tijaabooyin ama isbarbar dhigid taabasho ah si loo ogaado dhumucda lakabka ciidda lagu dahaadhay iyo dhumucda birta si loo xakameeyo heerka xoojinta ee ridaya. Tusaale ahaan, qaabeynta 490Q birta birta crankshaft birta caaryada geedi socodka shubista, dhumucda lakabka dusha sare ee ciidda waa 5-8mm, dhumucda derbiga ee caaryada birta waa 20-30mm, oo soo saarta tayo sare - sii dey birta aan duleelka lahayn. Sababta ugu weyn waa:
- Layer Lakabka ciidda ku dahaadhan wuxuu si wax ku ool ah u xakameeyaa heerka qaboojinta ee ridaha, dhinaca kale, wuxuu ka dhigayaa shubista inay u muuqato mid aan caddaan u muuqan, iyo dhinaca kale, heerka qaboojinta ayaa ka badan kan ciidda lagu ridayo. Sida ku cad Jaantuska 2, marka birta la shubay lagu shubo caaryada birta ku dahaadhan, heerkulka tuubista ayaa hoos u dhacaysa ilaa 930 ° C 8 daqiiqo ka dib, waxayna ku qaadataa 24 daqiiqadood caaryada ciiddu inay hoos ugu dhacdo isla heerkulka , iyo heerka qaboojinta waxaa lagu kordhiyay ilaa 3 jeer. Natiija ahaan, Waxyaabaha farsamooyinka ah ee castings si weyn ayaa loo hagaajiyay.
- Mold Caaryada birtu wax tanaasul ah ma leh, laakiin daaha ciidda khafiifka ah ayaa si ku habboon u yareyn karta caabbinta yareynta caaryada; iyo adkaanta caaryada birtu waxay si wax ku ool ah uga faa'iideysataa ballaadhinta garaafka birta dheecaanka ah inta lagu gudajiro geeddi-socodka xoojinta si loo gaadho No ridaya halista; bacaadka khafiifka ah awgood, daloolku ma fududa in la qalloociyo, saxsanaanta rida ayaa si weyn looga hagaajiyay ta caarada.
Laba shuruudood oo wareejinta kuleylka siday u kala horreeyaan oo matalaya xoojinta is-weydaarsiga kuleylka ee u dhexeeya ridaya iyo lakabka ciidda daboolan, iyo caaryada birta ah iyo lakabka ciidda daboolan. k1 waa saamiga u adkaysiga kuleylka ee ridaya ilaa caabbinta kuleylka ee daboolka ciidda; k2 waa saamiga u adkaysiga kuleylka ee nooca birta ilaa caabbinta kuleylka ee daboolka ciidda. Iyadoo la tixgelinayo isku darka k1 iyo k2, iyadoo la beddelayo dhumucda dusha sare ee ciidda, waxaa jira seddaxdan xaaladood ee kala-wareejinta kuleylka kala duwan ee u dhexeeya "ridaya-ciidda dahaarka-caaryada birta ah" ee run ahaantii dhici karta:
- Marka k≤1 iyo k2≤1, lakabka dusha sare ee ciiddu wuxuu ku dhex jiraa dhumucda caadiga ah, heerka qaboojinta ee ridaya ayaa sii kordheysa iyadoo dhumucda lakabka daaha ciiddu hoos u dhacayso.
- Markay dhumucda lakabka ciidda lagu dahaadhay ay dhaafto dhumuc cayiman, caaryada birtu wax saamayn ah kuma laha qaboojinta ridaha. Waqtigaan, waxay u dhigantaa ciida caadiga ah ee la tuurayo ama ridaha dhoobada. Maaddaama kuleylka kuleylka lakabka bacda leh uu aad uga yar yahay kan birta ah, shubku si tartiib ah ayuu u qaboobaa.
- HenMarka k ≧ 1 iyo k2 ≧ 1, dhumucda dusha ciidku aad ayuu u khafiifsan yahay, kaasoo u dhigma ka sameysma caaryada birta ah.
Sifooyinka sarrifka kuleylka ee kor ku xusan waxaa lagu xaqiijiyay tijaabooyin. Marka dhumucda lakabka bacda ee crankshaft (CTЦ-14) birta nooca-birta loo shubay si tartiib tartiib ah isu beddelo 4 ilaa 32 mm, qadarka sibidhka ee dhismaha crankshaft ayaa si isdaba joog ah loo dhimay, iyo xaddiga pearlite iyo The xaddiga ferrite ayaa sii kordhaya. Marka dhumucda lakabka ciidda lagu dahaadhay ay ka yar tahay 4mm, xoogga qaboojinta ee ridaya wuxuu la mid yahay kan birta ah (rinjiga qaro weyn); marka lakabka ciidda lagu dahaadhay uu ka weyn yahay 32mm, xoogga qaboojinta wuxuu u dhigmaa kan ridaya ciidda cusbi ee caadiga ah.
Marka loo isticmaalo kabka birta ah ee ku dahaadhan birta soosaarka noocyo kala duwan oo jilitaan ah, waa iyada oo loo marayo tijaabooyin ama isbarbar dhigid taabasho ah si loo ogaado dhumucda lakabka ciidda lagu dahaadhay iyo dhumucda birta si loo xakameeyo heerka xoojinta ee ridaya. Tusaale ahaan, qaabeynta 490Q birta birta crankshaft birta caaryada geedi socodka shubista, dhumucda lakabka dusha sare ee ciidda waa 5-8mm, dhumucda derbiga ee caaryada birta waa 20-30mm, oo soo saarta tayo sare - sii dey birta aan duleelka lahayn. Sababta ugu weyn waa:
- Layer Lakabka ciidda ku dahaadhan wuxuu si wax ku ool ah u xakameeyaa heerka qaboojinta ee ridaha, dhinaca kale, wuxuu ka dhigayaa shubista inay u muuqato mid aan caddaan u muuqan, iyo dhinaca kale, heerka qaboojinta ayaa ka badan kan ciidda lagu ridayo. Sida ku cad Jaantuska 2, marka birta la shubay lagu shubo caaryada birta ku dahaadhan, heerkulka tuubista ayaa hoos u dhacaysa ilaa 930 ° C 8 daqiiqo ka dib, waxayna ku qaadataa 24 daqiiqadood caaryada ciiddu inay hoos ugu dhacdo isla heerkulka , iyo heerka qaboojinta waxaa lagu kordhiyay ilaa 3 jeer. Natiija ahaan, Waxyaabaha farsamooyinka ah ee castings si weyn ayaa loo hagaajiyay.
- Mold Caaryada birtu wax tanaasul ah ma leh, laakiin daaha ciidda khafiifka ah ayaa si ku habboon u yareyn karta caabbinta yareynta caaryada; iyo adkaanta caaryada birtu waxay si wax ku ool ah uga faa'iideysataa ballaadhinta garaafka birta dheecaanka ah inta lagu gudajiro geeddi-socodka xoojinta si loo gaadho No ridaya halista; bacaadka khafiifka ah awgood, daloolku ma fududa in la qalloociyo, saxsanaanta rida ayaa si weyn looga hagaajiyay ta caarada.
Heerka Qaboojinta ee Iron Sand-Coated Castings
Waxyaabaha saameynaya heerka qaboojinta ee birta lagu dahaadhay ciidda birta waxaa ka mid ah dhumucda derbiga tuurista, wax shubka, kuleylka ku shubista, dhumucda cufnaanta ciidda, maaddada wax lagu dhejiyo ee ciidda ah, dhumucda caaryada birta ah, qalabka caaryada birta ah, iyo heerkulka caaryada. Halkan, kaliya saameynta tuurista dhumucda darbiga (bc), dhumucda dusha ciidka (bm) iyo dhumucda birta (bi) ayaa laga wada hadlay.
Saameynta bc, bm iyo bi On Qaboojinta Casting
Dhumucda darbiyada kala tuuraya ee kala duwan (10mm, 20mm, 40mm, 80mm, siday u kala horreeyaan), dhumucda ciidda oo kala duwan (4mm iyo 32mm, siday u kala horreeyaan) iyo dhumucda birta ee noocyada kala duwan (32mm iyo 8mm, siday u kala horreeyaan) oo lagu sameeyay xaaladaha soo socda ee tijaabada ah heerka qaboojinta ee noocyada birta ah ee birta ku dahaadhan birta: halabuurka kiimikada ee loo shubay waa 3.52% C, 2.46% Si, 0.80% Mn, 0.18% P, 0.031% S, iyo halabuurka kiimikada ee lakabka ciidda daboolan waa: 90% quartz sand, 8% dhoobo, Dhuxul budada 2%, qoyaan 3%
- Thickness Dhumucda darbiga tuurista, dhumucda dahaadhka ciidda iyo dhumucda gidaarka birta waxay saamaysaa heerka qaboojinta ee ridaya. Sidaa darteed, soosaarka dhabta ah, dhumucda caaryada birta ku habboon iyo dhumucda dusha sare ee ciidda waa in lagu xushaa iyadoo la raacayo dhumucda darbiyada tuuraya ee kala duwan si loo helo heerka qaboojinta loo baahan yahay.
- ② Tuurista dhumucda kaladuwan waxaa lagu heli karaa iyadoo la doorto dhumucda dusha sare ee ciidda iyo dhumucda gidaarka birta si loo helo isla heerka qaboojinta. Tusaale ahaan, Jaantuska 3, aaga I macnaheedu waa dhumucdiisuna waa 10mm iyo 20mm, aagga II waxaa loola jeedaa 20mm iyo 40mm, aagga IIIna waxaa loola jeedaa 40mm. Iyo iskudhafka udhaxeeya kala duwanaanta qaboojinta ee 80mm castings.
- In kasta oo bm iyo bi loo beddeli karo si loo helo isla heerka qaboojinta ee tuurista dhumucyada kala duwan, haddana dhumucda dhumucda oo dhan ma wada heli karaan heerka qaboojinta oo isku mid ah. Xaaladaha tijaabada awgood, shubista dhumucdiisuna tahay 10mm iyo dhumucdiisuna tahay 40mm lama heli karo Qiyaasta saxda ah ee qaboojinta (ma jiro wax isdhaaf ah oo u dhexeeya gooladaha).
Xulista Dhumucda Dahaarka Sand (bm) Iyo Dhumucda Birta Birta (bi)
Bm iyo bi guud ahaan waxaa lagu go'aamiyaa iyadoo lagu saleynayo khibrad ama tijaabo. Halkan waxaa ku yaal habka shaxanka, kaas oo ku habboon tuurista dhumucda (bc) laga bilaabo 10 illaa 80mm iyo soo deynta heerkulka 600 ℃. Wareegtu waa waqtiga qaboojinta. Abscissa qalooca dhinaca midig waxaa lagu calaamadeeyay dhumucda dusha ciida, taas oo lagu go'aamin karo waqtiga looga baahan yahay shubista la yaqaan si ay u qaboojiso ilaa 600 ° C iyo dhumucda tuubbada kala duwan, iyo dhumucda darbiga tuubbada loo baahan yahay (10, 20, 40, 80mm) waa la yaqaan, markaa aad ayey ugu habboon tahay in la go'aamiyo dhumucda dusha ciidda iyo dhumucda caaryada birta ah. Soo hel bc u dhigma (tusaale ahaan, bc = 20mm) xagasha jiifka ah ee qeybta bidix ee qallooca oo sawir xariiq jiifa.
Haddii labada sadar ay dhexgalaan inta u dhexeysa qalooca iskutallaabta, waxay muujineysaa in kabkaani ku habboon yahay Dheecaanka ciidda birta ah. Kordhi xariiqan jiifka ah midigta, waxayna u fidin doontaa aagga bc = 20mm, oo jiido xarriiq toosan oo aagga ah si aad u hesho dhumucda dusha sare ee ciidda loo baahan yahay. Si kastaba ha noqotee, xariiqan toosan waa in loo jiido dhinaca midig inta ugu macquulsan si loo helo dhumucda ugu yar ee bacaadka carrada iyo dhumucda caaryada birta ah. Haddii dhumucda lakabka bacaadka-ciidda ee u baahan in la go'aamiyo uusan ku jirin xadkaas, waxaad ka heli kartaa ka soo wareegidda qalooca ku dhow si la mid ah.
- Thickness Dhumucda darbiga tuurista, dhumucda dahaadhka ciidda iyo dhumucda gidaarka birta waxay saamaysaa heerka qaboojinta ee ridaya. Sidaa darteed, soosaarka dhabta ah, dhumucda caaryada birta ku habboon iyo dhumucda dusha sare ee ciidda waa in lagu xushaa iyadoo la raacayo dhumucda darbiyada tuuraya ee kala duwan si loo helo heerka qaboojinta loo baahan yahay.
- ② Tuurista dhumucda kaladuwan waxaa lagu heli karaa iyadoo la doorto dhumucda dusha sare ee ciidda iyo dhumucda gidaarka birta si loo helo isla heerka qaboojinta. Tusaale ahaan, Jaantuska 3, aaga I macnaheedu waa dhumucdiisuna waa 10mm iyo 20mm, aagga II waxaa loola jeedaa 20mm iyo 40mm, aagga IIIna waxaa loola jeedaa 40mm. Iyo iskudhafka udhaxeeya kala duwanaanta qaboojinta ee 80mm castings.
- In kasta oo bm iyo bi loo beddeli karo si loo helo isla heerka qaboojinta ee tuurista dhumucyada kala duwan, haddana dhumucda dhumucda oo dhan ma wada heli karaan heerka qaboojinta oo isku mid ah. Xaaladaha tijaabada awgood, shubista dhumucdiisuna tahay 10mm iyo dhumucdiisuna tahay 40mm lama heli karo Qiyaasta saxda ah ee qaboojinta (ma jiro wax isdhaaf ah oo u dhexeeya gooladaha).
Fadlan hayso isha iyo cinwaanka maqaalkan si dib loogu daabaco: Habka Iyo Codsiga Dahaarka Moldashiinka Mashiinka Caanka ah ee Sand-Coated
Minghe Shirkadda Die Casting waxaa ka go'an in ay soosaaraan oo ay bixiyaan Qaybo ka ridaya tayo iyo waxqabad sare (biraha qaybo ka ridaya dhiman kala duwan inta badan ka mid yihiin Khafiifa-Wall dhinta ridaya,Hot ridaya die Cast,Kursiga Qabow Die Casting), Adeeg Wareeg ah (Adeegga Tartanka Dhimashada,Qalabka Mashiinka,Samaynta Furka, Daaweynta Dusha sare) .Caadi kasta oo Aluminium ah shubitaan, magnesium ama Zamak / zinc shubida iyo shuruudaha kale ee shubanka ayaa lagu soo dhaweynayaa inaad nala soo xiriirto.
Iyada oo ay gacanta ku hayaan ISO9001 iyo TS 16949, dhammaan geeddi-socodyada waxaa lagu fuliyaa iyada oo loo marayo boqollaal mashiinno shub ah oo dhimanaya, mashiinnada 5-dhidibka, iyo tas-hiilaadka kale, oo ka bilaabma qarxiyayaal ilaa mashiinnada dharka lagu nadiifiyo ee Ultra Sonic.Minghe ma ahan oo keliya qalab casri ah laakiin sidoo kale waxay leedahay xirfadle koox injineero khibrad leh, wadayaal iyo kormeerayaal si niyada macaamiisha ay u noqoto mid run ah.
Soo saaraha qandaraasle ee shubka dhinta. Awoodda waxaa ka mid ah qaybaha qabow ee aluminium ee qaybaha shubista laga bilaabo 0.15 lbs. illaa 6 rodol, isbeddel deg deg ah oo la dejiyay, iyo qalabaynta. Adeegyada qiimaha lagu daro waxaa ka mid ah sifaynta, gariirka, qashin-qubka, xabbadda toogashada, ranjiyeynta, dahaadhka, dahaadhka, isku-ururinta, iyo qalabaynta. Qalabka lala shaqeeyay waxaa ka mid ah alloysyada sida 360, 380, 383, iyo 413.
Zinc wuxuu u dhintaa caawinta naqshadeynta / adeegyada injineernimada isku mar. Soo saaraha gaarka ah ee saxda saxda ah ee looxyada. Daarayaasha yar-yar, cast-yada u dhinta cadaadiska sare, jilayaasha caaryada badan-slide, shubka caaryada caadiga ah, cutubka dhinta iyo kuwa madaxa-bannaan ee loo dhinto iyo daloolka dahaarka saanlan ayaa la soo saari karaa. Jilayaasha waxaa lagu soo saari karaa dherer iyo ballac ilaa 24 gudaha. +/- 0.0005 gudaha. Dulqaad.
ISO 9001: soo saaraha shahaadada leh ee loo yaqaan 'cast cast magnesium', Awoodaha waxaa ka mid ah dhimista cadaadiska sare ee magnesium oo loo ridayo ilaa 2015 ton qol kulul & 200 ton oo qol qabow ah, naqshadeynta qalabka, nadiifinta, wax u sameynta, mashiinada, budada & dareeraha rinjiyeynta, QA buuxda oo leh awooda CMM , ururinta, baakadaha & gaarsiinta.
ITAF16949 la xaqiijiyay. Adeeg Dheeraad Dheeraad ah Ayaa Kujira maalgelinta maalgelinta,ciida ciid,Dabaaldeg Shaqo, Casting Foam Fost,Khadka Centrifugal,Dabka Vacuum Casting,Qaab Joogtada ah, Awoodda waxaa ka mid ah EDI, kaalmada injineernimada, qaabeynta adag iyo ka shaqeynta heerka labaad.
Warshadaha Kabka Qaybaha Daraasada Kiiska ee loogu talagalay: Gawaarida, Baaskiiladaha, Diyaaradaha, Qalabka muusikada, Biyaha, Qalabka indhaha, Dareemayaasha, Moodooyinka, Aaladaha elektarooniga ah, Xiritaanka, Saacadaha, Mashiinnada, Mashiinnada, Qalabka guryaha, Dahabka, Jigs, Telecom, Laydhka, Qalabka Caafimaadka, Qalabka Sawirka, Robotyo, farshaxanno, qalabka codka, Qalabka isboortiga, Qalabaynta, Caruurta iyo waxyaabo kale oo badan.
Maxaan kaa caawin karnaa inaad sameyso marka xigta?
Tag bogga hore ee loogu talagalay Shiinaha dhinta Casting
→Qeybaha kabkaOgow waxaan soo qabanay.
Tips Tilmaamaha Halaasiga ah ee Ku Saabsan Adeegyada Cast Cast
By Soo saaraha Minghe Die Casting | Qeybaha: Maqaallo waxtar leh |Waxyaabaha Tags: Casting Aluminium, Tuurista Zinc, Ridaya Magnesium, Qalitaanka Titanium, Qalabka birta ee birta, Naxaas naxaas ah,Raxaama Naxaas,Video Tuuraya,Taariikhda Shirkadda,Calaamadda Aluminum Die Casting | Faallooyinka Off