Waxyaabaha Sababa Dhimashada Qalabaynta Qalabka
Sababaha Dildilaaca
- Heerkulka caaryada ayaa aad u sarreeya inta lagu gudajiro geedi socodka wax soo saarka dhinta-shubka (waxaa ugu wanaagsan in lagu daro nidaamka qaboojinta).
- Wakiilka sii deynta caaryada waxaa lagu buufiyaa si aan macquul ahayn inta lagu gudajiro geedi socodka wax soo saarka dhinta-shubka.
- Daaweynta kuleylka caaryada ah maahan mid ku habboon, badanaa sababtoo ah adkaanta (adkaanta waa inaysan ka yareyn HRC-47).
- Qalabka birta caaryada ah ma fiicna, waxaa lagugula talinayaa inaad isticmaasho 8407 ama H13 la safeeyey
Dildilaaca hore wuxuu guud ahaan sabab u yahay heerkulka foojignaanta badan ee foojignaanta maran (oo badanaa loo yaqaan 'overburning'). Kordhinta xad-dhaafku waa cillad aan laga soo kaban karin, sidaa darteed heerkulka been abuurka ah inta lagu gudajiro nidaamka waxsoosaarka maran waa in si adag loo xakameeyo. Isla waa isku mid geedi socodka deminta. Waqtiga kululaynta waa in si adag loo xakameeyo si looga hortago in la burburiyo. Maaddada kadib markii la xusho, waa daaweyn kuleyl. Qadar cayiman oo wax soo saar ah ka dib, fiiro gaar ah u yeelo yareynta buufiska. Sidoo kale, naqshadeynta waa inay ahaato mid macquul ah, iskuday inaad ka fogaato feejignaanta walbahaarka, oo fiiro gaar ah u leeg cabirka xagasha R. Qiyaastii 10,000 jeer oo caaryo ah, caaryadu waa inay fiiro gaar ah u yeelato dabciga si looga saaro buuqa. Culeyska haraaga ah ee ka-shaqeynaya xoog-ku-uruurinta xoogga gudaha lama saaro. Cadaadiska kuleylka ee geedi socodka dhimashada-si fiican looma saarin. Marka la soo koobo, dildilaaca ayaa ah waxqabadka isku-buuqa diiqadda. Waxaad isticmaali kartaa xanaaqa badan si aad uga saarto diiqada. Waxay kordhin kartaa nolosha caaryada.
Sababaha ugu waaweyn ee loo jeexjeexayo wasakhda aluminium ee wasakhda u dhinta-qaadista ka dib muddo wax soo saar waa sidan soo socota:
- Heerkulka caaryadu aad ayuu u sarreeyaa welwelkuna aad buu u weyn yahay
- Qalabka udub-dhexaadka ah wuxuu adeegsadaa 8407, skd61
- Daaweynta kuleylka caaryada ee adag ayaa aad u sarreeya
- Dayactir joogto ah, 5k jeer1 tempering, 15k times1 tempering 30k times.
Si looga hortago in caaryada dhinta-ridaya ay dillaacdo oo ay kordhiso nolosha adeegga caaryada, qodobbada soo socda waa in la sameeyaa:
- 1. Daaweynta kuleylka ee qaybta sameynta ee caaryada dhinta-tuurista (dhaqaaqa, xudunta go'an, xudunta) waxay u baahan tahay in adkaanta loo dammaanad qaaday inay noqoto HRC43 ~ 48 (maaddadu waxay noqon kartaa SKD61 ama 8407)
- 2. Caaryadu waa in si buuxda loo kululeeyaa inta aan la soo saarin wax dhinta, oo shaqooyinkeeduna waa sida soo socota:
- 2.1 Ka dhig caaryada inay gaarto dheelitir wanaagsan kaamerada, ka dhig mid isku mid ah heerka adkeynta tuurista isla markaana fududeyso gudbinta cadaadiska.
- 2.2 Joogtee dareeraha isku-darka dhinta-kabka markii la buuxiyo, yeela qaab wanaagsan oo hagaajiya tayada dusha sare ee ridaya
- 2.3 In la yareeyo cilladaha soo-saarka ka hor iyo in la hagaajiyo wax-soo-saarka dadka dhinta.
- 2.4 Iska yaree culeyska kuleylka ee kuleylka isla markaana kordhiya nolosha adeegga caaryada.
Faahfaahin gaar ah waa sida soo socota:
Nooca Alwaax | Qaab kululaynta heerkulka (℃) |
Aluminum Daawaha | 180 ~ 300 |
Zinc Daawaha | 150 ~ 200 |
Ka dib markii caaryada cusub la soo saaro muddo, isku ururinta diiqada kuleylka ayaa ah sababta tooska u ah dillaaca asaasiga caaryada. Si loo yareeyo culeyska kuleylka, udub-dhexaadka caaryada iyo slider ka dib muddo cayiman ka dib waa in la xakameeyaa si looga takhaluso cadaadiska kuleylka. Qaababka wax soo saarka gaarka ah ee u baahan in laga tirtiro buufiska kuleylka waa sida soo socota:
Nooca Maqalka | Aluminum Daawaha | Zinc Daawaha |
Cadaadiska Koowaad | <2000 jeer | <10000 jeer |
Dabeecad Labaad | <10000 jeer | <20000 jeer |
Dabeecadda Saddexaad | <30000 jeer | <50000 jeer |
Qalabka aluminium ee aluminiumku wuxuu udub dhexaad u yahay culeyska shaqada, waana in fiiro gaar ah loo yeesho qalabka caaryada, qaabeynta, farsamaynta, daaweynta kuleylka iyo qalliinka si loo helo nolol dheer oo caaryo ah. Kuwa soo socdaa waa 25 talooyin oo loogu talagalay sameynta caaryadu inay gaarto nolol dheer:
- Qalab tayo sare leh
- Naqshad macquul ah ee dhumucda derbiga caaryada iyo cabirrada kale ee caaryada ah
- Isku day inaad isticmaasho waxyaabaha la gelinayo
- Xulo geeska ugu weyn ee suurtogalka ah R markay suurtagal tahay
- Masaafada u dhexeysa kanaalka biyaha qaboojinta iyo muuqaalka iyo geeska waa inuu ahaadaa mid ballaaran
- Cadaadiska culeyska fekerka iyo xanaaqa waa in la sameeyaa ka dib qallajinta xun
- Daaweynta kuleylku waa sax, oo deminta iyo qaboojinta waa inay ahaadaan kuwo deg deg ku filan
- Si fiican u nadiifi oo ka saar lakabka metamorphic EDM
- Dusha sare laguma safeyn karo
- Dusha sare ee caaryada waa in lagu qayilaa
- Haddii nitriding xulasho ah, lakabka dhex-dhexaadintu waa inuusan noqon mid aad u qoto dheer
- Ku kululey caaryada heerkulka lagu taliyey sida saxda ah
- Xawaaraha gaagaaban oo gaabis ah waa in loo adeegsadaa in lagu bilaabo dhimista-shubka 5-10 gogo '
- Iska yaree heerkulka aluminiumka la shubay sida ugu macquulsan ee ku aaddan helitaanka alaab tayo leh
- Ha isticmaalin xawaaraha duritaanka aad u sarreeya ee dareeraha aluminium
- Hubso in caaryada si fiican loo qaboojiyey, iyo heerkulka biyaha qaboojinta waa in lagu hayaa 40 ~ 50 ℃
- Xiritaanka ku meel gaarka ah, iskuday inaad xirto caaryada oo aad yareyso qadarka biyaha qaboojinta si looga fogaado shoog kuleylka ku dhaca caaryada markii dib loo bilaabayo
- Qaboojiyaha waa in la demiyaa marka dusha moodeelka uu ku jiro heerkulka ugu sarreeya
- Ma aha wakiilka sii deynta buufin badan
- Kadib qadar cayiman oo dhimasha ah, walaaca oo yaraada iyo xanaaq
- Sababta ugu weyn ayaa ah in heer kulku aad u sareeyo. Waxaa lagugula talinayaa inaad isticmaasho heerkulbeeg si loo xakameeyo heerkulka wakhti kasta inta lagu gudajiro geerida shubista (heerkulka lagu taliyay ee aluminiumka aluminiumka u dhinta-shubka waa <650)
- U fiirso kuleylka kuleylka ah si looga hortago daalka kuleylka. (Dildilaaca waxaa badanaa keena daalka kuleylka)
- Fiiro gaar ah u yeelo wax soo saarka caaryada, waxaa ugu wanaagsan in la isticmaalo xarun wax lagu farsameeyo si loo dhammaystiro, haddii ay jirto baahi loo qabo farsameynta korantada, ka dib marka la sameeyo korantada, shiidi iyo nidaamyada wax safeeya waa in lagu daraa.
- Fiiro gaar ah u yeelo dayactirka caaryada (yareynta walaaca iyo xanaaqa)
- Waxaa lagugula talinayaa inaad u isticmaasho ASSAB 8407 qaab-dhismeedyada leh baahiyo nololeed oo sarreeya, adkeysiyada wasakhda dhinta ayaa lagu talinayaa inaysan ka sarreynin 50HRC
Fadlan hayso isha iyo cinwaanka maqaalkan si dib loogu daabaco:Waxyaabaha Sababa Dhimashada Qalabaynta Qalabka
Minghe Shirkadda Die Casting waxaa ka go'an in ay soosaaraan oo ay bixiyaan Qaybo ka ridaya tayo iyo waxqabad sare (biraha qaybo ka ridaya dhiman kala duwan inta badan ka mid yihiin Khafiifa-Wall dhinta ridaya,Hot ridaya die Cast,Kursiga Qabow Die Casting), Adeeg Wareeg ah (Adeegga Tartanka Dhimashada,Qalabka Mashiinka,Samaynta Furka, Daaweynta Dusha sare) .Caadi kasta oo Aluminium ah shubitaan, magnesium ama Zamak / zinc shubida iyo shuruudaha kale ee shubanka ayaa lagu soo dhaweynayaa inaad nala soo xiriirto.
Iyada oo ay gacanta ku hayaan ISO9001 iyo TS 16949, dhammaan geeddi-socodyada waxaa lagu fuliyaa iyada oo loo marayo boqollaal mashiinno shub ah oo dhimanaya, mashiinnada 5-dhidibka, iyo tas-hiilaadka kale, oo ka bilaabma qarxiyayaal ilaa mashiinnada dharka lagu nadiifiyo ee Ultra Sonic.Minghe ma ahan oo keliya qalab casri ah laakiin sidoo kale waxay leedahay xirfadle koox injineero khibrad leh, wadayaal iyo kormeerayaal si niyada macaamiisha ay u noqoto mid run ah.
Soo saaraha qandaraasle ee shubka dhinta. Awoodda waxaa ka mid ah qaybaha qabow ee aluminium ee qaybaha shubista laga bilaabo 0.15 lbs. illaa 6 rodol, isbeddel deg deg ah oo la dejiyay, iyo qalabaynta. Adeegyada qiimaha lagu daro waxaa ka mid ah sifaynta, gariirka, qashin-qubka, xabbadda toogashada, ranjiyeynta, dahaadhka, dahaadhka, isku-ururinta, iyo qalabaynta. Qalabka lala shaqeeyay waxaa ka mid ah alloysyada sida 360, 380, 383, iyo 413.
Zinc wuxuu u dhintaa caawinta naqshadeynta / adeegyada injineernimada isku mar. Soo saaraha gaarka ah ee saxda saxda ah ee looxyada. Daarayaasha yar-yar, cast-yada u dhinta cadaadiska sare, jilayaasha caaryada badan-slide, shubka caaryada caadiga ah, cutubka dhinta iyo kuwa madaxa-bannaan ee loo dhinto iyo daloolka dahaarka saanlan ayaa la soo saari karaa. Jilayaasha waxaa lagu soo saari karaa dherer iyo ballac ilaa 24 gudaha. +/- 0.0005 gudaha. Dulqaad.
ISO 9001: soo saaraha shahaadada leh ee loo yaqaan 'cast cast magnesium', Awoodaha waxaa ka mid ah dhimista cadaadiska sare ee magnesium oo loo ridayo ilaa 2015 ton qol kulul & 200 ton oo qol qabow ah, naqshadeynta qalabka, nadiifinta, wax u sameynta, mashiinada, budada & dareeraha rinjiyeynta, QA buuxda oo leh awooda CMM , ururinta, baakadaha & gaarsiinta.
ITAF16949 la xaqiijiyay. Adeeg Dheeraad Dheeraad ah Ayaa Kujira maalgelinta maalgelinta,ciida ciid,Dabaaldeg Shaqo, Casting Foam Fost,Khadka Centrifugal,Dabka Vacuum Casting,Qaab Joogtada ah, Awoodda waxaa ka mid ah EDI, kaalmada injineernimada, qaabeynta adag iyo ka shaqeynta heerka labaad.
Warshadaha Kabka Qaybaha Daraasada Kiiska ee loogu talagalay: Gawaarida, Baaskiiladaha, Diyaaradaha, Qalabka muusikada, Biyaha, Qalabka indhaha, Dareemayaasha, Moodooyinka, Aaladaha elektarooniga ah, Xiritaanka, Saacadaha, Mashiinnada, Mashiinnada, Qalabka guryaha, Dahabka, Jigs, Telecom, Laydhka, Qalabka Caafimaadka, Qalabka Sawirka, Robotyo, farshaxanno, qalabka codka, Qalabka isboortiga, Qalabaynta, Caruurta iyo waxyaabo kale oo badan.
Maxaan kaa caawin karnaa inaad sameyso marka xigta?
Tag bogga hore ee loogu talagalay Shiinaha dhinta Casting
→Qeybaha kabkaOgow waxaan soo qabanay.
Tips Tilmaamaha Halaasiga ah ee Ku Saabsan Adeegyada Cast Cast
By Soo saaraha Minghe Die Casting | Qeybaha: Maqaallo waxtar leh |Waxyaabaha Tags: Casting Aluminium, Tuurista Zinc, Ridaya Magnesium, Qalitaanka Titanium, Qalabka birta ee birta, Naxaas naxaas ah,Raxaama Naxaas,Video Tuuraya,Taariikhda Shirkadda,Calaamadda Aluminum Die Casting | Faallooyinka Off