Waxyaabaha Sababa Dildilaaca Kulaylka iyo Qabowga Marka la tuurayo Shaagagga
Giraangiraha aluminium ee aluminiumku waxay leeyihiin astaamo badan oo giraangiraha biraha aysan iswaafajin karin. Sidaa darteed, giraangiraha aluminium aluminium ayaa si ballaaran loogu isticmaalay gawaarida, mootooyinka iyo gawaarida kale. Markay ahayd 2002, xaddiga rarka ee giraangiraha aluminium ee baaburta Shiinaha wuxuu ku dhowaaday 45%. Sababtoo ah shuruudaha tayada sare leh ee giraangiraha gawaarida, qaab dhismeedkeedu wuxuu ku habboon yahay tuurista saxda ah ee cadaadiska hooseeya, dalabkuna waa weyn yahay, wuxuu si weyn kor ugu qaaday horumarinta tiknoolajiyada tuurista hooseeya. Waqtigan xaadirka ah, tuurista cadaadiska hoose ayaa noqotay habka ugu muhiimsan ee habka wax soo saarka aluminium giraangiraha aluminiumka ah, inta badan Shiinaha soosaarayaasha aluminiumka aluminium ee Shiinaha waxay u adeegsadaan nidaamkan wax soo saar.
Dildilaaca cadaadiska hooseeya ee tuurista aluminium aluminium aluminium badanaa waxaa sababa feejignaanta walaaca, ama dildilaaca ay keento xoog aan sinnayn marka xarunta laga saaro, ama dareeraha ku adkaada tuubada kacsan. Dildilaaca guud ahaan waxaa loo qaybiyaa dildilaacyo qabow iyo dildilaacyo kulul.
Dildilaaca qabow waxaa loola jeedaa dillaacyada la sameeyay markii ay daawaha ka hooseeyaan heerkulkiisa adag. Marka la eego shuruudaha laymanka, dildilaaca qabow waxaa sababa marka saxsanaanta dajinta saxitaanka ee ku shaqeysa shandadku ay ka sarreyso heerka ay oggoshahay xoogga ama baaxadda balastarka laftiisa marka si sax ah loo qaboojiyo heerkul hoose. Dildilaaca qabow badanaa wuxuu ka muuqdaa dusha sare ee kabka, oo leh qiiqa yar ee dusha dildilaaca; halka dildilaaca kulul badanaa loo tixgeliyo inuu yahay mid la soo saaray inta lagu gudajiray adkeynta aaladda. Wareejinta kuleylka darbiga caaryada dartiis, ridayaashu had iyo jeer waxay bilaabaan inay ka adkaadaan dusha sare. Marka tiro fara badan oo laamood ahi ay ka soo baxaan dusha sare ee ridaha oo ay is dul saaran si ay u samaystaan qalfoof dhammaystiran, shubistu waxay u muuqan doontaa hoos u dhac ku yimaada xaalad adag (oo badanaa loo muujiyo hoos u dhigid toosan).
Si kastaba ha noqotee, wali waxaa jira lakab filim bir ah oo dareere ah (filim dareere ah) oo u dhexeeya dendrites waqtigaan. Haddii hoos u dhigidda shubista aan la hor istaagin, lakabka dendrite saameyn kuma yeelan doono xoog wuxuuna u yaraanayaa si xor ah, mana muuqan doono. cadaadis. Marka yaraanshaha lakabka dendrite-ka la carqaladeeyo, si xor ah uma yarayn karo ama wuxuu ku hoos jiraa ficil xoog xoog leh, culeys fiiqan ayaa soo muuqan doona. Waqtigaan, filimka dareeraha ah ee udhaxeeya dendrites waa la beddeli doonaa iyadoo la fidinayo.
Marka culeyska culeyska culus uu ka bato xadka xoogga filimka dareeraha ah, dendrites waa la kala jiidan doonaa. Si kastaba ha noqotee, weli waxaa jira biro dareere ah oo ku wareegsan qaybta dillaacday. Haddii filimka dareeraha ah si tartiib tartiib ah loo kala jiido oo ay jiraan dareere ku filan hareeraha oo uu ku qulqulo qaybta dillaacsan waqtiga, qaybta dillaacsan ayaa la buuxin doonaa "wayna bogsan doontaa". Wax soo saarka saxda ah ee saxda ah ma muujin doono dildilaacyo kulul. Haddii dildilaaca silsiladdu aaney mar kale "bogsan karin", dildilaacyo kulul ayaa ka soo muuqan doona wax soo saarka saxda ah. Dusha sare ee jabka kuleylka ah ayaa si xoogan oksijiin u leh, oo muujinaya midab madow ama madow oo aan lahayn dhalaal bir ah.
Fadlan hayso isha iyo cinwaanka maqaalkan si dib loogu daabaco:Waxyaabaha Sababa Dildilaaca Kulaylka iyo Qabowga Marka la tuurayo Shaagagga
Minghe Shirkadda Die Casting waxaa ka go'an in ay soosaaraan oo ay bixiyaan Qaybo ka ridaya tayo iyo waxqabad sare (biraha qaybo ka ridaya dhiman kala duwan inta badan ka mid yihiin Khafiifa-Wall dhinta ridaya,Hot ridaya die Cast,Kursiga Qabow Die Casting), Adeeg Wareeg ah (Adeegga Tartanka Dhimashada,Qalabka Mashiinka,Samaynta Furka, Daaweynta Dusha sare) .Caadi kasta oo Aluminium ah shubitaan, magnesium ama Zamak / zinc shubida iyo shuruudaha kale ee shubanka ayaa lagu soo dhaweynayaa inaad nala soo xiriirto.
Iyada oo ay gacanta ku hayaan ISO9001 iyo TS 16949, dhammaan geeddi-socodyada waxaa lagu fuliyaa iyada oo loo marayo boqollaal mashiinno shub ah oo dhimanaya, mashiinnada 5-dhidibka, iyo tas-hiilaadka kale, oo ka bilaabma qarxiyayaal ilaa mashiinnada dharka lagu nadiifiyo ee Ultra Sonic.Minghe ma ahan oo keliya qalab casri ah laakiin sidoo kale waxay leedahay xirfadle koox injineero khibrad leh, wadayaal iyo kormeerayaal si niyada macaamiisha ay u noqoto mid run ah.
Soo saaraha qandaraasle ee shubka dhinta. Awoodda waxaa ka mid ah qaybaha qabow ee aluminium ee qaybaha shubista laga bilaabo 0.15 lbs. illaa 6 rodol, isbeddel deg deg ah oo la dejiyay, iyo qalabaynta. Adeegyada qiimaha lagu daro waxaa ka mid ah sifaynta, gariirka, qashin-qubka, xabbadda toogashada, ranjiyeynta, dahaadhka, dahaadhka, isku-ururinta, iyo qalabaynta. Qalabka lala shaqeeyay waxaa ka mid ah alloysyada sida 360, 380, 383, iyo 413.
Zinc wuxuu u dhintaa caawinta naqshadeynta / adeegyada injineernimada isku mar. Soo saaraha gaarka ah ee saxda saxda ah ee looxyada. Daarayaasha yar-yar, cast-yada u dhinta cadaadiska sare, jilayaasha caaryada badan-slide, shubka caaryada caadiga ah, cutubka dhinta iyo kuwa madaxa-bannaan ee loo dhinto iyo daloolka dahaarka saanlan ayaa la soo saari karaa. Jilayaasha waxaa lagu soo saari karaa dherer iyo ballac ilaa 24 gudaha. +/- 0.0005 gudaha. Dulqaad.
ISO 9001: soo saaraha shahaadada leh ee loo yaqaan 'cast cast magnesium', Awoodaha waxaa ka mid ah dhimista cadaadiska sare ee magnesium oo loo ridayo ilaa 2015 ton qol kulul & 200 ton oo qol qabow ah, naqshadeynta qalabka, nadiifinta, wax u sameynta, mashiinada, budada & dareeraha rinjiyeynta, QA buuxda oo leh awooda CMM , ururinta, baakadaha & gaarsiinta.
ITAF16949 la xaqiijiyay. Adeeg Dheeraad Dheeraad ah Ayaa Kujira maalgelinta maalgelinta,ciida ciid,Dabaaldeg Shaqo, Casting Foam Fost,Khadka Centrifugal,Dabka Vacuum Casting,Qaab Joogtada ah, Awoodda waxaa ka mid ah EDI, kaalmada injineernimada, qaabeynta adag iyo ka shaqeynta heerka labaad.
Warshadaha Kabka Qaybaha Daraasada Kiiska ee loogu talagalay: Gawaarida, Baaskiiladaha, Diyaaradaha, Qalabka muusikada, Biyaha, Qalabka indhaha, Dareemayaasha, Moodooyinka, Aaladaha elektarooniga ah, Xiritaanka, Saacadaha, Mashiinnada, Mashiinnada, Qalabka guryaha, Dahabka, Jigs, Telecom, Laydhka, Qalabka Caafimaadka, Qalabka Sawirka, Robotyo, farshaxanno, qalabka codka, Qalabka isboortiga, Qalabaynta, Caruurta iyo waxyaabo kale oo badan.
Maxaan kaa caawin karnaa inaad sameyso marka xigta?
Tag bogga hore ee loogu talagalay Shiinaha dhinta Casting
→Qeybaha kabkaOgow waxaan soo qabanay.
Tips Tilmaamaha Halaasiga ah ee Ku Saabsan Adeegyada Cast Cast
By Soo saaraha Minghe Die Casting | Qeybaha: Maqaallo waxtar leh |Waxyaabaha Tags: Casting Aluminium, Tuurista Zinc, Ridaya Magnesium, Qalitaanka Titanium, Qalabka birta ee birta, Naxaas naxaas ah,Raxaama Naxaas,Video Tuuraya,Taariikhda Shirkadda,Calaamadda Aluminum Die Casting | Faallooyinka Off